Warning: Undefined property: stdClass::$canonical in /home/assdaasn/public_html/components/com_rsblog/views/post/view.html.php on line 162

Stainless Opulence

Stainless Opulence

Exemplary stainless steel craftmanship has delivered a sophisticated and lavish cocktail lounge in the heart of the Gold Coast’s entertainment hub.

Cocktail connoisseurs have been flocking to Cherry, The Star Gold Coast to experience the designer drinks on offer in the grandeur of the lounge featuring a 22m long bar. Refurbished in 2017 as part of the first stage of the property’s major transformation, its upmarket look and feel was inspired by its sister venue at The Star Sydney.

Central to Cherry’s luxury design is the intricate, gold metalwork featured in the VIP booth screens, lounge surrounds and balustrades. ASSDA Member and Accredited Fabricator Minnis & Samson fabricated these elements using grade 316 stainless steel tube and flat bar supplied by ASSDA Member Australian Stainless Distributors

The stainless steel was mirror polished prior to the electrostatic application of a special coating to achieve the gold colour finish. Crystal hardware and lush red velvet furnishings complement the gold stainless steel to deliver the opulent design and vision of the cocktail lounge.

Stainless steel is a high quality and high strength material, and was specified for its longevity, hygienic properties and aesthetic appeal. In addition, stainless steel offered better weldability to achieve the detail in the metalwork’s curvature design.

This article featured in Australian Stainless magazine - Issue 63, Spring 2018