Logo


Immerse yourself in stainless luxury

Setting the benchmark in boutique luxury and innovation using stainless steel is Brisbane’s Emporium Hotel.

Developed by the Anthony John Group, The Emporium Hotel opened in July 2018. Nestled in the premier lifestyle and cultural precinct of South Bank, the 143-suite hotel is turning heads with its exquisite interior design, bespoke handcrafted features and luxurious facilities.

Stainless steel was the material of choice for the five-star hotel and selected for its quality, opulent aesthetic and luxury appeal. Over 5.5 tonnes of grade 304 stainless steel sheet, 1.2mm thick in a No. 8 mirror finish was used throughout the five-star hotel and supplied by ASSDA Member Fagersta Steels

ASSDA Member and Accredited Fabricator, Langford Metal Industries, was engaged to laser cut the mirror finish material to bring the developer’s trademark design to life, which was installed by Thump Architectural.

The frangipani inspired pattern represents the Queensland theme and character, and the laser cut stainless steel prevails throughout the hotel on mullions, sliding doors, external panels, columns, cabana suites surrounding the 23m infinity edge pool – almost anywhere and everywhere, serving both a functional and decorative purpose.

A remarkable feature of the hotel is its rooftop bar on the 21st floor, The Terrace. Presenting panoramic views of South Bank Parklands, the Brisbane River and the city skyline, The Terrace maximises the warm Queensland weather with two retractable roofs offering full, partial or no exposure.

Measuring 7.5m long, 2.1m wide and 50mm thick, the ceiling of the first retractable roof features the impressive frangipani stainless steel design. The sliding panel is a composite structure incorporating insulation and structural members which are clad top and bottom with mirror polished stainless sheet. For structural purposes, the panel was shaped into a shallow moon profile to form the roof’s arch. When retracted, a second roof made of glass is revealed, which is also retractable for a complete outdoor rooftop experience.

The stainless steel ceiling and surrounding elements complement the rooftop bar’s sub-tropical luxe vibe with ceiling-to-floor glass doors, lush greenery, and white backlit onyx floor tiles and bar.

 

Photo Credit: Emporium Hotel

Coastal living

Stainless Steel Pool Fencing

Safety is the number one consideration when building a pool fence, and stainless steel delivers in compliance and material strength while fulfilling design and aesthetic needs.

A stunning canal-front home on the Gold Coast features a streamlined stainless steel vertical balustrade system as supplied by ASSDA Member Miami Stainless.

The custom-designed stainless steel pool fence features 50mm square mirror-polished posts and upper and lower rails. Complying with Queensland pool fencing and safety barrier regulations, the vertical stainless steel wire balustrades were spaced 80mm apart and installed using Miami Stainless’ Nutsert Swage Stud System on the base with a ProRig Flip Toggle into the handrail.

Grade 316 stainless steel was specified for its aesthetic appeal, material strength and corrosion resistance, particularly with the home’s waterfront location and close proximity to the coastline.

In addition, stainless steel is a durable and long-lasting alternative to aluminium balustrades and offers reduced household maintenance when compared with glass. Glass fencing often requires frequent cleaning to remove chlorine or saltwater splashes and finger marks. 

The stainless steel pool fence ticks all the boxes in combining safety, unobstructed views, durability, minimal maintenance and luxury style.

 

Photo credit: Miami Stainless

 

Stainless Steel and Fire Resistance

What is the fire rating of stainless steel? This is a common enquiry from ASSDA Members and the construction industry, especially with the current concerns about flammable cladding. The three major branches to this question are covered in this article.

 Will stainless steel burn, and if it does, will it give off fumes or facilitate the spread of fire?  

This question is readily answered because stainless steels are steels. It is recognised that steels do not burn and only start to melt at about 1400oC. This means that stainless steels do not have a “fire rating” as such, so the tests of AS/NZS 1530.3 (or the equivalent tests in BS 476) are not required.

Heating in a fire will obviously have an appearance effect because, unlike the transparent nanometer-thick passive layer formed in moist air, stainless steels heated above about 300oC in air discolour as they grow a less dense oxide layer. This develops from the rainbow colours seen beside welds to a dark and non-protective oxide layer whose thickness depends on the time of exposure and temperature reached. The street rubbish bin shown suffered from a fire but remained functional for almost a year (until the repair cycle reached it) with a decorative rainbow oxide. By way of comparison, powder coated bins would suffer from unsightly burn marks and corrosion. 

For austenitic alloys such as 304 and 316, the temperature limits for lifetime section loss due to oxidation is about 870oC (with temperature cycling) so they are routinely used in high temperature furnaces and ductwork. The current trend to apply decorative coatings to stainless steels would require an assessment to determine the combustibility, potential fumes and flame spread of the coating. Tests to AS/NZS 1530.3 would be appropriate. 

Microstructural effects of a short-term heat cycle (less than a couple of hours of exposure, such as a fire) could include carbide precipitation (sensitisation) in an austenitic alloy which was not an L grade (i.e. carbon >0.03%). Duplex and weldable ferritic grades should not have sufficient carbon for sensitisation. Sensitisation would degrade the corrosion resistance but not affect mechanical properties. Both duplex and ferritic grades can suffer 475oC embrittlement, however data produced by the International Molybdenum Association (IMOA) shows that this requires more than two hours in the 400oC to 500oC range for a 50% reduction in toughness. This duration is unlikely in most fires.

 

Will stainless steel provide a barrier to flames and if it does, how rapidly will the heat penetrate the barrier sufficiently to cause damage (usually a specific temperature rise) on the far side? 

A satisfactory demonstration is supplied by reference BS 647 Part 22 tests carried out for a British Stainless Steel Association (BSSA) member, Stewart Fraser, who manufacture 316 framed doors which include a cavity filled with non-combustable boards. The results are given at www.bssa.org.uk/topics.php?article=106.

It showed slight discolouration and distortion on the flame impingement side with the sheltered side of the door reaching only 98oC after 60 minutes. The test was continued for another 80 minutes without the failure of flame containment or subsequent opening of the door in its frame. Similar testing was carried out on a 1.5mm thick 2304 duplex sheet fabricated into a simulated ship’s bulkhead with enclosed ceramic wool insulation. With a bright orange glow of an 1100oC metal temperature on the flame side, the “safe” side reached 30oC after 40 minutes and 110oC after 60 minutes. The test was terminated after 120 minutes with containment still satisfying IMO resolution A518 (XIII).

 

What are the effects (both during and after an event) to the mechanical properties of stainless steel? How do these compare with structural carbon steels? 

There are tests as well as a theoretical basis which demonstrate that both austenitic and duplex stainless steels have superior high temperature properties compared to carbon steel. The table below shows the deflection and failure modes of three metre long commercial electrical cable trays loaded to simulate actual loadings. They were heated with 18 LPG burners to obtain an average temperature of 1000oC  to 1050oC for at least five minutes. [Nickel Institute publication No. 10042]

    

 

The publication also considers the life cycle costs (LCC) of the use of aluminium, galvanised steel or stainless steel for stairways, handrails, gratings and firewalls, as well as cladding for corridors and accommodation modules on North Sea platforms. Fire risk controls are obviously a major concern although corrosion resistance is also critical. On an LCC basis, stainless steel was most economical especially when its reduced requirement for maintenance periods were included. 

In addition to the above testing in cable tray applications, substantial research and application work has since been carried out and codified. Installations include 2205 duplex hangers suspending the slab which forms the floor of the emergency ventilation duct in the CLEM7 tunnel in Brisbane [ISSF].

In short term fires such as on balconies or stairways, the temperature rise exposed to an ISO 834 fire temperature profile depends on thickness and emissivity. Polished stainless steels typically have low emissivity of <0.1 and hence a slower temperature rise. Conservatively, after 30 minutes a 12mm sheet of stainless steel with 0.2 emissivity would reach 620oC whereas steel (with no rust) and 0.4 emissivity would reach 750oC.   

When considering strength and deflection, the metal temperatures in a conventional fire do not reach levels to anneal the material so any cold work strengthening will raise the temperature for a 50% strength reduction. In addition, as shown in the graph, the reduction in Young’s Modulus, i.e. deflection from a specific load, is less than that of carbon steel for temperatures above ~200oC. By 600oC the modulus retention for stainless steel is 0.75 compared to 0.3 for carbon steel, i.e. less than half the deflection for a given load.

 

         

 

In summary, stainless steel has substantial advantages in structural use when fire risk is considered, and these advantages continue into higher strength and lower deflections at elevated temperatures.

CLEM7 image above courtesy of Ancon.

This article is featured in Australian Stainless Magazine issue 65, 2019.

 

 

 

Grand Reflections

Innovative Melbournian architecture has delivered a striking stainless steel feature in the city’s latest commercial mixed-use development.

Melbourne is setting the benchmark for world-class design with Collins Square now one of Australia’s largest CBD commercial precincts, covering an entire city block on Collins Street. Already home to a number of leading global corporations and the revitalised heritage-listed Southern Goods Shed, the $2.5 billion project will at completion comprise of five commercial towers and over 10,000sqm of retail space.

Black mirror finish stainless steel columns are the focal point in the lobbies and food precincts of Towers Two and Four of Collins Square. Soaring an impressive 10m to 12m tall at a diameter of 1300mm, the stainless steel-clad columns are complemented by floor-to-ceiling window glass and natural stone masonry walls and floors.

ASSDA Member Fabmetal Specialists supplied, fabricated and installed the grade 304 stainless steel circular columns, using its own patented column cladding system. Twenty stainless steel clad columns were installed across the two towers.

Fabmetal Specialists’ pre-fabricated the customised stainless steel column panels from 1.2mm sheet, and using a modular cladding method, installed the panels with a unique fixing system allowing no visible fixings or caulked joints.

Coloured stainless steel in a No. 8 mirror finish from the company’s TiVox range was used for the project and specified for its upmarket appeal and elegant aesthetics. In addition, stainless steel also offers durability and ease-of-use during construction.

Providing a true mirror reflection, the black chromatic colour (known as ‘Jet Mirror’ in the TiVox range) was achieved with a titanium film using a Physical Vapour Deposition (PVD) coating process. The coating technology offers a number of high chemical and technical features, including resistance to abrasion, scratches and corrosion, and overall minimal maintenance.

The end result is an innovatory, high quality stainless steel finish, bringing life to the surrounding activity of Melbourne’s place-to-be for business and leisure.

This article featured in Australian Stainless magazine - Issue 62 Winter 2018.

 

Stainless Sustains Intricate Brick Facade

Stainless steel is playing a vital role in the structural integrity of a new state-of-the-art library at one of Brisbane’s most prestigious boys’ school.

The Centenary Library at Anglican Church Grammar School was designed by Brand + Slater Architects, and the ambitious project was part of the school’s master plan to provide a technology-rich, world-class centre for its 1800 students. Comprising four levels, the tertiary-inspired building features an extensive range of learning spaces including a 250-seat lecture theatre, teaching and meeting rooms and over 80 individual study areas.

The library stands 23.5m tall on a heritage-listed part of the school campus. Paying homage to the school’s history whilst appealing to a contemporary aesthetic, the library exterior features an intricate brick façade backed by a stainless steel support and restraint system custom-designed and manufactured by ASSDA Member and Accredited Fabricator, Ancon.

Grade 304 stainless steel was used and specified for its longevity, durability and performance properties to meet the building’s 50+ year design life.

Ancon’s specialist knowledge, manufacturing agility and project management service proved invaluable to the contractor when building the detailed façade of the decorative arches and corbelled brickwork with all structural steelwork now unseen.

Shelf Angle Brick Support

Ancon masonry support systems enabled the large-scale brick cladding installation on this impressive education facility to be completed to the highest safety standards, while showcasing its architectural brickwork features.

Ancon’s MDC and CFA continuous shelf angle support systems carry the intricate brick façade, consisting of freestanding archways and projected brickwork. The MDC stainless steel angles are fixed to the reinforced concrete frame, span a 40mm cavity, and create a horizontal shelf to provide the necessary support for up to 3 metres of brickwork.

Cast-In Channel

Ancon’s 30/20 cast-in horizontal channels were used to provide the fixing between the concrete frame and shelf angles. The channel enabled the necessary horizontal adjustment for the installer, and its compact size eliminated the issue of potential clashes with the reinforcement steel in floor slabs.

Nail holes aided the fixing of channels to timber framework and an infill prevented the ingress of concrete during casting. Cast-in fixings do not generate expansive forces in concrete. It can therefore be used at close centres and often used closer to the edges than expansion fittings.

Wall Ties and Restraint Fixings

To restrain the distinctive brickwork details to the reinforced concrete structure, stainless steel L-shaped SPB and SDB frame cramps were fixed into the reinforced concrete using 6mm FBN expansion bolts.

FBN single expansion bolts are a cost-effective anchor and fix into a hole similar to the diameter of the bolt. This allows the hole to be drilled through the hole in the item to be fixed.

Technical Expertise

As part of Ancon’s free design service, plans were produced illustrating the location and reference of all fixings required. Ancon’s early engagement with the project’s structural engineers, Bligh Tanner, enabled a workable and cost-effective design to be agreed upon prior to the build of the complex masonry features. Sharing their expertise with the clients at this stage of the project meant installation difficulties, site delays and unnecessary remedial measures were avoided.

  

 

Centenary Library photo (above); Copyright: Christopher Frederick Jones.

This article is featured in Australian Stainless Magazine #61.

Art Symbolises Community

You return home after a long journey. Imagine being greeted by a beautiful stainless steel sculpture surrounded by landscaped gardens on your return. One ASSDA Member has used stainless steel to symbolise everything we love about our communities: Security, comfort and home.

It’s easy to think of stainless steel in relation to tubes, panels and rolls in the construction industry, but Brisbane-based ASSDA member, Concept Stainless Design, has taken the product and crafted it into stunningly beautiful sculptures for developers Villa World at their new subdivision on the northern Gold Coast.

Located 70km south of Brisbane, Arundel Springs will provide 386 dwellings in a family-friendly environment adjacent to the Coombabah Lakelands Conservation Area and close to Griffith University and light rail services.

Villa World provided the concept design to reflect the organic growth of nature and symbolise the new families and children who will grow in the new suburb. 

The team at Concept Stainless Design adapted the design to match the size of available grade 316 stainless steel sheets. A small curve of 5mm radius was provided at the tip of the fronds to avoid sharp edges. Another small curve of 9mm was used at the gully between fronds to achieve a flawless polished finish.

The sculptures have been designed to withstand winds of up to 160km per hour, an important feature given Arundel Spring’s proximity to the ocean. An internal frame was built to secure the fronds in position, as well as a horizontal base beam hidden within the sculpture and two legs extending down from the base beam into a large buried concrete block. The structural design certification was completed by Concept Stainless Design’s in-house engineer.

The face of each sculpture was manufactured from grade 316 stainless steel sheet supplied by ASSDA Sponsor Dalsteel Metals.

The sculpture faces are joined along the centre line with an invisible polished butt weld, executed by Concept Stainless Design’s highly skilled tradesman at their Brisbane workshop. The faces were bonded to marine ply and “U” stiffeners were formed from grade 316 stainless steel strips then glued and screwed in. The second face was then placed over the stiffeners, glued and screwed to the ply-bonded face.

The entire project took eight weeks to construct and transported to their new home at Arundel Springs. The sculptures were secured in place by concrete blocks and steel bolts provided by Villa World’s civil contractor in under two hours.

Stainless steel was chosen for the sculptures because of its beautiful, smooth and highly polished finish, and for its low-maintenance properties. Surrounded by clear skies, new vegetation and lush grass, the sculptures welcome residents and visitors alike.

This article is featured in Australian Stainless Magazine Issue 60 (Summer 2017/18).

Impressive Stainless Steel Ribbon Graces New Brisbane Food Gallery

Stainless steel has brought life to a unique food precinct located in a recently opened premium office tower in Brisbane City's Golden Triangle.

Developed and constructed by Grocon, 480 Queen Street’s sustainable and eclectic design boasts a 6 Star Green Star and a 5 Star NABERS rating. The building’s food gallery, otherwise known as Room 480, is located on level 2 and capitalises on the stunning views of Brisbane River and Story Bridge to deliver a restaurant style experience and retreat for diners.

Complementing this space is a suspended stainless steel sculpture, designed by local architecture and interior design practice Arkhefield. Inspired by water flowing around rocks, the ‘stainless steel ribbon’ delicately hangs from the ceiling and weaves over the landscape of the room.

Grade 304 stainless steel was specified for the ribbon feature, using 100m of 0.9 x 600mm coil supplied by ASSDA Sponsor Dalsteel Metals. The 1 tonne of coil was supplied in a Bright Annealed (BA) finish and polyethylene coating on both sides for protection, with one side brighter than the other to fulfill the architectural effect and design requirements.

Arkhefield wanted the ribbon feature to be highly reflective on one side, with a brushed appearance on the other. As it curves and wraps through the space, the bright and flat sides of the stainless steel ribbon interact to reflect the surrounding colours and light, allowing movement and distortion throughout. Stainless steel proved the only material able to achieve this aesthetically appealing finish, whilst providing a high-quality, durable and lightweight structure.

The stainless steel ribbon spans 35m x 6m across Room 480’s ceiling and was installed by ASSDA Member and Accredited Fabricator Stainless Aesthetics.

Stainless Aesthetics Director Mike Mooney said the installation of the entire 1 tonne of stainless steel coil as a continuous ribbon was one of the more challenging aspects of the project. This was successfully achieved using their custom designed and fabricated turntable, which housed the coil and allowed it to unwind safely 3.5m above floor level, while protecting the ribbon’s surface finish.

The installation of the stainless steel ribbon around the light fixtures emphasised the visual appeal of the sculpture and its surface qualities. It is suspended using 3.2mm wire support cables and fixings in grade 316 stainless steel supplied by ASSDA Member Anzor Fasteners.

The stainless steel ribbon is an impressive and visually dynamic integrated element of Room 480, adding colour and movement to a traditionally formal space. In addition, the sculpture provides a level of intimacy to the space that could not be achieved with a standard flat suspended ceiling, providing a pleasant ambience for patrons to dine and relax.

This article is featured in Australian Stainless Issue 57 (Spring 2016).

Images courtesy of Stainless Aesthetics.

Stainless Steel Design Innovation

Brisbane’s iconic Story Bridge is sporting increased safety measures with the application of innovative stainless steel products and laser-fusion technology.

 The 76-year old heritage-listed cantilever bridge now incorporates three-metre tall, stainless steel safety barriers on its pedestrian walkways, as a result of an outstanding collaboration between multiple project stakeholders. Completed in December 2015, the $8.4 million project was led by design and construct head contractor, Freyssinet.

The design brief was to develop an anti-climb structure that was both functional and aesthetically appealing, whilst ensuring the heritage values of the bridge were maintained.

This presented a number of engineering challenges, including the affixation of the barrier structure to the existing heritage-listed bridge without permanent methods of attachment, such as welding or other damaging techniques, whilst addressing the weight and wind load tolerances, ambient vibrations and noise potential.

Visually, there was also a key design requirement to ensure pedestrian views of the river, Brisbane city and surrounds, and of the Story Bridge itself, was preserved.

The initial reference design was specified in stainless steel (with an option for painted carbon steel) and required the fabrication of heavy box sections for over 1000 posts to support a tamper-resistant, horizontal balustrade cable system. The outrigging was specified in carbon steel, with isolation joints to support the upright posts. However, aesthetically, this design created a clutter of vertical elements.

Freyssinet developed an alternative design concept employing Carl Stahl X-TEND® stainless steel mesh, and engaged ASSDA Member Ronstan Tensile Architecture to assist in the design rationalisation. Ronstan Tensile Architecture conducted form-finding analysis to mimic increasing the mesh self-span between the posts. The findings resulted in a substantial reduction in the number of posts required and a more secure fall-restraint system than initially designed.

Replacing the original tension wire design with a mesh barrier significantly reduced the structural loading on the posts, allowing for a smaller number of lighter duty posts, and reducing the cost below the initial estimate.

The concept solution delivered was a dynamic structural design that met the exacting demands of the specification. The design evolved to using laser-fused stainless steel open section beams for the posts, positioned approximately three metres apart with a blackened Carl Stahl X-TEND® stainless steel mesh barrier.

This project is the largest to date in Australia using laser-fused stainless steel structural beams.

Low impact laser-fusion is a process that allows the welding together of pre-polished flat components to a special profile without damaging the visible surface. It provides an effective and economical alternative to extrusions or conventional welds, providing closer tolerances, superior joint integrity and more consistent finishes.

The introduction of laser-fused stainless steel structural beams into the Australian market allowed Freyssinet the flexibility to plan and design with stainless steel in an outcome that was unrivalled for the project scope. Developed and manufactured by Montanstahl (Switzerland) and its subsidiary Stainless Structurals Asia (Singapore), the laser-fused stainless steel structural beams were supplied by ASSDA Sponsor Atlas Steels, as the exclusive agent for the product in Australia.

To this end, Atlas Steels supplied over 30 tonnes of stainless steel for the project, including 316L grade 80x80x6mm I-beam sections for the 530 upright posts, 316 grade 65x65x6mm angle bars for the outrigging, and 316 grade 38.1x1.6mm 320 grit polished tube for the framing of the mesh.
The I-beams supplied were made from a pre-polished strip with a <0.5Ra finish. The I-beam components were laser cut, polished, and then laser-fused together.

Freyssinet rolled the I-beams using a local roll forming company in Eagle Farm to form a curve, following several prototypes to achieve the required design. The beams were then delivered to ASSDA Accredited Fabricator Stainless Engineering Services to cut the posts to the specified height, verify the dimensions, placement and drilling of the holes for the bolt connections, and passivate the posts to ASTM 380 prior to installation.

Stainless Engineering Services also used the offcuts from the I-beams to fabricate the brackets, ensuring no material wastage.

ASSDA Member Anzor Fasteners supplied 550 units of grade 316 stainless steel coupling cables in various lengths of up to 2.1 metres, in 4mm diameter and 1/19 configuration. Each cable was swaged to a threaded stud on one end and a u-shaped fork coupling on the other end. The coupling cables were used to affix the X-TEND mesh to the posts, providing an adjustable method of attachment.

Following the erection of the posts, Ronstan Tensile Architecture supplied and installed 3400m2 of Carl Stahl X-TEND® 316 grade stainless steel mesh constructed from coloured stainless steel wire rope. The stainless steel was blackened with an additional polyester amino resin, which was hardened to the wire under temperature.

The blackened Carl Stahl X-TEND® mesh was the key to achieving an unobtrusive composition and historical aesthetic, while providing the flexibility and tensile strength required for the structure’s design and use of the laser-fused posts.

The structure is a pivotal safety addition to the Story Bridge and exudes functionality in its excellent and unique engineered design. Stainless steel is unmatched in the materials selection for providing durability, structural performance, low maintenance, corrosion resistance and aesthetics.

This article is featured in Australian Stainless Issue 56 (Winter 2016).

Photography by Fullframe Photographics.

Stainless in Color

A modern and innovative design using coloured and textured stainless steel has left an impressive statement on an Adelaide streetscape.

South Australia’s premier shopping district Rundle Mall underwent a full makeover from 2012-2014 as part of the Adelaide City Council’s initiative to revitalise the precinct.

Part of this redevelopment included a redesign of the facade of a commercial tower at 80 Grenfell Street, housing the Adelaide headquarters of the Bendigo and Adelaide Bank.

Design practice HASSELL delivered an iridescent façade design using coloured stainless steel cladding, supplied by ASSDA Member Steel Color Australia. The extent of the façade referred to as ‘the ribbon’ cascades over 10 storeys, connecting the office tower to the lobby entrance via the retail parapet. The ribbon was made up of over 100 panels that twist and bend over the full height of the building, creating an artistic ripple effect.

HASSELL and Arup’s façade engineering team tested this unique design with physical and virtual models, further refining the design detailing with extensive prototyping. This collaboration with the assistance of Steel Color Australia’s product and material knowledge ensured this remarkable design element was feasible.

Stainless steel was specified for this design as its inherent properties allowed for the level of manipulation required to construct the architect’s creative expression, as well as provide a high quality and aesthetically pleasing finish.

Over 1500m2 of grade 304 stainless steel in 4000x1250x1.2mm sheet in a Rosso colour (Italian for red) was supplied by Steel Color Australia, as the sole distributor in Australia and New Zealand for embossed, coloured, mirror finished and textured stainless steel manufactured by Steel Color S.p.a in Italy.

Steel Colour Australia owner Vince Araullo said that electro-colouring (INCO system) is the main technology in Steel Color Australia’s production. ‘The stainless steel sheet’s surface was directly altered, chemically stimulating the natural passivation of the material. No painting was involved in the process, increasing the pitting resistance of the stainless steel.’

In terms of manipulating the steel’s shape, Araullo said that colouring is an intrinsic part of the stainless steel. ‘This means the stainless does not lose colour during shaping, as opposed to aluminium for example which would need to be coloured after folding due to the fragility of the coloured anodic coating.’

Steel Color Australia facilitated the overseas production of some 270 sheets, weighing 10 tonnes and their shipment to the project site. Modular framework was constructed to bend the stainless sheets into shape for easy installation on site by crane.

The visually striking building façade integrates impressively into the Rundle Place precinct, and the outcome has resulted in a virtually maintenance-free and colour enduring structure.

This article is featured in Australian Stainless Issue 56 (Winter 2016).

Images courtesy of Steel Color Australia.

Stainless Steel Leads a Stellar Redevelopment

When Sydney's Star City Casino emerged from the chrysalis of its construction scaffolding, its metamorphosis included a gleaming 340m2 stainless steel-and-glass canopy facing the harbour.

ASSDA member and Accredited Fabricator TripleNine Stainless fabricated and installed the canopy over the main entrance of ‘The Star’, as it is now known, as part of an $850 million redevelopment. This transformation saw Sydney’s only casino swing its orientation 180° from Pyrmont’s fish markets toward the city’s glittering Darling Harbour.

The Star’s façade was designed by Fitzpatrick + Partners and is comprised of 147 flags of clear, low-iron glass supported by two fingers of 20mm and 166mm plate stainless steel. The surfboard-shaped canopy is 40m x 8.5m and made of 300 nominal bore pipe with a lattice effect created by 100 x 50 rectangular hollow sections. All 18 tonnes of stainless steel is 316 grade and was supplied by ASSDA sponsor, Atlas Steels.

Peter Petro, the site architect for the project, says stainless steel was the obvious choice from both a practical and an aesthetic point of view. ‘From a practical perspective, we chose stainless steel because it’s so close to the water and we needed something that was resilient.’

In terms of aesthetics, Petro says they wanted a high-quality finish for the front of the building and stainless steel was a prime choice. ‘We also had a lot of lighting design so we wanted something that would bounce the light around. We were able to give the stainless steel a polish that also matched the glass façade upstairs. This gives it a playfulness at night and a high finish during the day.’

TripleNine’s Director, Justin Brooks, says electropolishing wasn’t an option because of the massive size of the canopy. ‘Instead, it was polished to 400 grit then passivated with an Avesta product.’

Brooks says the project's engineers and designers, Yuanda, employed a Feng Shui expert to sign off on the canopy before
it was built at TripleNine’s purpose-hired workshop. ‘The basic geometry came from the client but we did the design detailing because of all the different shapes and angles,‘ explains Brooks.

The $1.4 million canopy project commenced in August 2010 and was completed in January 2011 with about 15 people assigned to the project. The canopy was built in one piece and transported with a police escort in the dead of the night on the back of a truck with front and rear steering. Installation took only two days, says Brooks.

During the design-detailing phase, TripleNine employed 3-D modelling and Yuanda’s engineers gave careful consideration to expansion and
contraction. ‘Because [the canopy] was so big, we needed to include some bridge building technology,’ says Brooks. ‘We used expansion pads as the canopy was calculated to expand up to 50mm across the total length of it.’

‘The Star’ is a bright, light addition to the harbourside landscape. While the elements of Feng Shui can’t be guaranteed to produce financial fortune in The Star’s casinos, the stainless steel canopy is certain to maintain its appeal for decades to come.

Images courtesy of TripleNine Stainless.

This article is featured in Australian Stainless, issue 52.

Reflected Glory

Stainless steel’s star has ascended in the public’s conscience as thousands of Westfield Sydney shoppers enjoy the world-class design and materials on show in its newest retail development.

Covering 103,000m2, the $1.2 billion Westfield Sydney development is bound by the Pitt Street Mall and Market and Castlereagh Streets in the heart of Sydney’s CBD. It integrates Westfield Centrepoint, the Centrepoint Convention Centre, Imperial Arcade and Skygarden, plus a new office tower at 85 Castlereagh Street and an extensively modified and refurbished tower at 100 Market Street.

While the size of the project is enormous, it’s the design that’s turning heads. With a nod to lauded international developments in Paris and Frankfurt, the architects of Westfield Sydney have created a stunning environment that makes extensive use of mirror and hairline finished stainless steel in the interior spaces.

Stainless steel was chosen by Westfield’s architects to create a very upmarket, stylish environment for shoppers. In addition to meeting the design intent, stainless steel also offers durability and ease-of-use during construction.

ASSDA Accredited Townsend Group was chosen to design, fabricate and install stainless steel elements throughout the complex, a task it was confident to undertake due to its experience delivering exceptional quality products to exacting clients, such as Apple Inc.

Townsend was awarded the following elements using only 316 grade stainless steel:

›    8,500m2 of mirror-finished stainless steel troughs and particle board infills in the feature ceilings on levels 3 and 4
›    Composite stainless steel panel cladding of the escalators on all levels
›    Black glass and mirror-finished stainless steel on the escalator soffits in void 4
›    Hairline-finished stainless steel composite panel cladding in voids 1 to 10
›    Mirror-finished stainless steel cladding of the elliptical column in void 1 from levels 1 to 5.

The project’s innovative design and engineering required the use of Townsend’s Vee-Cutter, the only one of its type in Australia, to create a very tight radii on the corners on some of the architectural elements. No additional services or treatments were required before or after installation as the stainless steel was procured with a protective film that remained on the product through the manufacturing process until the installation was complete.

Townsend Managing Director and CEO Russ Hill stated that the company was excited when selected for this prestigious development. The complexity of the project presented many challenges which Townsend was able to meet through its skill and experience, resulting in a finish which met the brief set by Westfield and its architects.

Images courtesy of Townsend Group.

This article is featured in Australian Stainless magazine - Issue 50, Summer 2011/12.

Stainless Strengthens Walls

The devastation of the 1989 Newcastle earthquake resulted in a revision of standards specifying building materials and products to be used in differing environments. 

One of the products that came under close scrutiny was wall ties (also known as brick ties).

Assessment of the damage after the earthquake found that many walls had 'peeled away' from building structures due to deteriorated wall ties.

A wall tie connects masonry to the structural backing which supports the wall. The most common wall ties are manufactured out of galvanised steel.

Australian Standard AS 3700 - 1998 revised the conditions under which wall ties are used and made recommendations about the types of material that should be used in different environments.

The Standard specifies that 316 or 316L stainless steel wall ties should be used in 'R4' category environments. These are severe marine environments, usually up to 1 00 metres from a nonsurf coast or one kilometre from a surf coast, where the highest airborne salinity level at the exterior of the masonry is 300 g/m2/day.

In such environments the chlorides in the air make it highly corrosive and not suitable for wall ties manufactured from materials that are susceptible to corrosion.

However this requirement is the subject of debate, with some specialists suggesting that corrosive environments stretch well beyond the distances specified in the Standard.

The use of stainless steel wall ties as suggested in the Standard will increase the safety and durability of buildings in corrosive environments for a very small increase in the overall cost. This again leads to the debate about what constitutes a corrosive environment, and whether the Standard should be more conservative.

The revised Standard has been incorporated into the Building Code of Australia and is mandatory for many provisions in the Code. The Australian Building Codes Board anticipates AS3700 - 1998 will become mandatory for the Housing Provisions in January 2000.

Thus, opportunities exist for the stainless industry to be proactive in its approach to such issues, as well as to investigate the use of stainless in other building applications, where durability and strength are principal concerns.

This article featured in Australian Stainless magazine - Issue 13, May 1999.

Chifley stands the test of time

Sydney's recently redeveloped Chifley Square now pays tribute to its namesake in a dramatic, yet personable, manner - an 8m tall stainless steel sculpture of Ben Chifley towers over the square, forming part of City of Sydney's capital works program in the lead up to the Sydney 2000 Olympics.

Chifley_3Sydney artist Simeon Nelson designed 'Ben Chifley' and a glass and stainless steel wall on the site while working as part of the multi-disciplinary design team involved in the site's $3 million redevelopment. Hassell architects (Sydney) were given open guidelines for the design of the site, but two of the objectives were to see Chifley appropriate recognised and to provide a windbreak on the Hunter Street side of the square.

Nelson specified 5 tonnes of 20mm grade 316 stainless plate for two cut-out images of the former war-time treasurer and the post-war Labor prime minister. The plates are positioned in parallel and bolted to a stainless frame, allowing 1mm tolerances.

Nelson designed the sculpture in stainless steel because of its long-term durability. He also felt the material was appropriate because it is often used as an industrial product and Chifley kick-started industrial growth after the war.

The sculpture was fabricated by CBD Prestige Metal Works (Sydney) from material supplied by Sandvik Australia (Smithfield, NSW). After shotblasting by IMP (Sydney), the final surface finishing and passivating was carried out by BHM Stainless Technology Group (Keon Park, Vic) using a specialised process developed by the company for unusual projects of this nature.

Chifley_wallSimilarly impressive is the 'Lightwall, Crucimatrilux' (also fabricated by CBD), which incorporates panes of transparent glass bolted together on nine stainless frames made of 74mm x 20mm bar with a mill finish. Because of the fine tolerances required, dowel and glue were used instead of welds to hold the frames together.

The 10.8m long and 3.2m tall wall serves a structural function as an extension of the back wall of the cafe and also acts as a wind shelter. visually, it provides a contrast with cafe's wall, which is made from white coated glass.

The redevelopment of the site, which is semi-circular in shape and divided in half by Philip Street, was aimed at unifying the two spaces to reflect the original intent of the site's 1937 design. Together, the Lightwall and Chifley sculpture form part of an impressive, contemporary response to historic town planning.

This article featured in Australian Stainless Issue 11, March 1998.

Everlasting Trees Reflect a Shade of Christmas

As we pack up our Christmas decorations, vow to lose those extra kilos gained over the holidays and make plans for the new year, the festive season seems so long ago - not so far for travellers and pedestrians on St Kilda Road in Melbourne.

Perched in front of Central Equity's three new apartment buildings are 12 three metre tall stainless steel trees which, although not specifically designed as Christmas trees, have stylised conical shapes that have a distinctly Christmas 'feel' about them.

Central Equity commissioned Phillip Naughton of Design Inferno to design the trees to complement the prestigious $123 million complex.

"Trees were specifically chosen for the design to reflect the living trees on the boulevard in front of the building," Mr Naughton said.

"They also add a human element to the complex. Because the buildings are 24 stories high, the architects, the Span Group, paid close attention to the surrounding landscape to ensure that they would not be imposing.

"We worked closely with the Span Group when designing the trees so that they would add to the feel of the complex," Mr Naughton said "In fad, unless you look straight up, you don't realise the scale of the buildings because their surrounds are so comfortable."

Stainless steel was chosen for the design for its inherent qualities.

"The design brief specified that the trees had to be low maintenance. Stainless steel fitted this brief as well as adding other qualities such as simplicity and the sense of movement that could be achieved through different surface finishes," Mr Naughton said.

"As one side of each tree is mirror finished, with the other side satin finished, they reflect the seasonal colours of the living trees on the boulevard. They have changed from reflecting little colour through the winter months when the deciduous trees were without leaves, to reflecting the lush green growth of spring."

According to Joe Delacruz of DBM Industries, the trees' fabricator, welding was the most difficult aspect of the fabrication.

"The design of the trees made them susceptible to buckling during welding," Mr Delacruz said.

"To add to the difficulty, the welds had to be invisible."

As part of the careful planning for the job, DBM first built scale models of the trees from timber.

The trees were laser cut and mirror finished at DBM Industries' facility at Reservoir in Victoria. ASSDA members MME Surface Finishing of Seaford in Victoria did the satin finish.

Each tree is made from approximately 400 kilograms of grade 316 stainless steel sheet set into a concrete base which is covered with a 20mm base plate. They are capped with 10 x 30mm capping. ASSDA members Atlas Steels supplied the stainless for the job.

The trees are located on 150 metres of streetscape on St Kilda Road (near the intersection of Toorak Road).

This article featured in Australian Stainless magazine - Issue 15, February 2000.

Let the Games Begin!

When millions around the world watch the Sydney Olympic Games this September, they will also be experiencing the best of Australian architecture, with particular emphasis on stainless steel.

Stadium Australia, located at Homebush Bay in Sydney's inner city in the centrepiece of the Olympic site. Here, events such as the opening and closing ceremonies and the track and field program will be played out. Closer examination of the sit reveals the use of stainless steel in a myriad of applications, both aesthetic and functional. Perhaps more importantly, the use of stainless steel helps meet the organiser's "green" commitment: to use materials with minimal impact on the environment and designs that reduce waste and conserve resources.

THE STADIUM
Seating 110,000, Stadium Australia is the largest stadium in the history of the Olympic Games. To give an idea of its size, the two main curved trusses span 296 metres and four Boeing 747s would fit side by side under the span of the main arch.

The roofing material was supplied by ASSDA member Atlas Steels (Australia) Pty Ltd, the handrails by ASSDA member Sandvik Australia.

Nineteen lighting towers, representing the number of cities in which the Olympic Games have been held to date, stand like sentinels guarding the entrance to Stadium Australia.

The towers consist mostly of concrete and painted steel, but grade 316 stainless steel rods, 25 millimetres in diameter, provide tension in each corner, while 316 doors and infill panels, with a No. 4 finish, exist at ground level.

The names of each of the cities where the Games have been held are glass-bead blasted on to grade 316 sheet with a No. 4 finish.

These towers each carry solar panels that contribute to the public elecricity grid an amount of power equal to that consumed by the towers at night.

At the bottom of one of the towers is a Munich Memorial to honour the athletes who died at the 1972 Munich Olympics. The memorial consists of three plaques fabricated from grade 316 stainless steel and glass, the names being engraved and paint filled in a surface with a No. 4 finish. Stainless steel channel sections, glass bead blasted on the inside and mirror polished were used around some of the edges.

Spread over six levels, the kitchens at Stadium Australia will see almost as much action as the field! Anticipated to feed about 110,000 people every day during competition, the kitchens have been fitted out with stainless steel equipment including benches, exhaust hoods, 200 deep-fat fryers and 300 upright refrigerators. ASSDA members Curtin Foodservice Equipment Pty Ltd supplied a bulk of the equipment, including over four and a half kilometres of stainless steel benches, 145 stainless steel hi-velocity extraction hoods, 200 deep-fat fryers, bain maries, refrigeration equipment, bulk and plated hot food holding carts and more than 200 mobile trolleys. Grade 304 stainless steel for the equipment was provided by ASSDA member Fagersta Steel.

THE OLYMPIC VILLAGE
Home to 15,000 athletes, officials and coaches during competition, the Olympic Village reflects stainless steel's contribution to the "Green Games". 6,000 kilograms (10,500 square metres) of grade 316 stainless steel mesh were installed to provide a chemical-free termite barrier to over 500 houses in the Village.

Fabricated and installed by Termi-Mesh Sydney Pty Ltd, the stainless steel mesh provides a physical barrier around the building perimeter and is collar clamped to pipes and other entry points. The result is a permanent obstruction to termites that eliminates the use of potentially dangerous chemicals.

OLYMPIC BOULEVARD
Olympic Boulevard, which passes key venues such as Stadium Australia and the Aquatic Centre, features spectacular fountains with stainless steel components.

Water jets, each covered by a grade 316 stainless steel cowl, provide a cascading arch at Fig Grove.

Fabricated grade 316 stainless steel gratings, black chrome plated so they are almost invisible under water, are used as safety screens. Grade 316 sections are also used to ensure the water cascades evenly along the length of the feature and as structural supports.

At the far end of the Boulevard is a fountain featuring lines of tubular water jets. Each jet comprises an inner structure of grade 316 stainless steel tubes clad with 3 millimetre thick 316 sheet, formed into a tapered cylindrical section with a No. 4 finish.

The underground pump house receives fresh air through spiral, welded ducting consisting of 250 millimetre diameter grade 316 stainless steel. A nearby wooden viewing pier has 316 handrails on galvanised steel uprights.

THE TORCH
Perhaps the most evocative symbol of the Games is the Olympic Torch, which carries the flame from Olympia in Greece to Stadium Australia, via the Olympic Torch Relay.

he design of the approximately 1 kilogram, 72 centimetre tall torch includes three layers representing earth, fire and water. The inner layer is polished stainless steel, the middle layer anodized aluminium and the outer layer specially coated aluminium.

Thin grade 316 stainless steel strip was used to form a skin inside the grade 430 stainless steel tube inner layer, acting as a shield against heat, wind and rain. Also, very fine (25 micron opening) 316 stainless steel gauze was installed as a final filter to clean the liquid propane/butane gas mixture that fuels the torch, thereby preventing contaminants from extinguishing the flame.

The torch was fabricated by Sydney firm GA & L Harrington, who produced over 14,000 torches available for purchase by the 10,000 runners participating in the Torch Relay.

This article featured in Australian Stainless magazine - Issue 16, August 2000.

Stainless Welcome for Sports Fans

Sports fans trekking to Melbourne's Colonial Stadium will enter the ground via a 200 metre long, 20 metre wide bridge shrouded in stainless. 

The Bourke Street Pedestrian Bridge, which connects Spencer Street Station to the eastern entrance of the $460 million sporting arena, opened in March 2000, makes extensive use of stainless steel to stunning effect.

A 200 metre long canopy comprising 14 rolled cascading stainless steel sheets divided in sections by red coated curved steel antlers protects pedestrians queuing on the south side of the bridge. The antlers, made from carbon steel, provide lighting and primary support to the stainless steel canopy.

400 metres of stainless steel handrailing with balustrades run the length of each side of the bridge.

he bridge connects the Gateway to the east and adjacent Spencer Street Station and extends across the station to the West End Connection above North-South Road.

Pedestrians entering the 30 000 person capacity bridge on the station side are greeted by two red glass towers, large staircases and a crushed wall of stainless steel through which a ramp connects disabled access from street level to the bridge.

Wood Marsh, the firm commissioned to design the bridge, said stainless steel was chosen because of its appearance, low maintenance and longevity.

"With thousands of people expected to cross the bridge every time an event is on, we needed a material that would not only withstand this level of traffic, but would make an eye-catching entrance to the stadium."

"Stainless steel was the obvious material choice -it is durable, needs limited upkeep and achieved the look we were after."

The roof cladding consists of 20 tonnes of 1.6mm grade 316 stainless steel sheets rolled to a radius of approximately 325mm butt joined, with a No. 4 finish to both faces.

400 metres of 6 inch, Sched 40 grade 316 stainless steel pipe was used for the handrails, polished to a No. 4 finish.

The handrails were constructed at Shearform Industries' workshop and installed, invisibly fixed, on site. The roof cladding was fabricated and polished in the workshop and installed on site.

The roofing material was supplied by ASSDA member Atlas Steels (Australia) Pty Ltd, the handrails by ASSDA member Sandvik Australia.

This article featured in Australian Stainless magazine - Issue 17, January 2001.

Stainless Export Defies Elements

Sixty tonnes of stainless steel has been exported to Hong Kong as part of an innovative Australian-designed and manufactured kit form, large span skylight project worth three quarters of a million dollars. 

The 42 gable trussed skylights and sub-frames in varying sizes up to four metres wide and eight metres long were installed in a $90 million dollar treatment plant commissioned by the Hong Kong Government.

Grade 316 stainless steel was used for the skylight's precision pre-cut sub-frame members, welded maintenance ladders, lntalok mechanism assemblies, special profiles, on sight assembly jigs, pivots and fixings.

The project specified that the skylights be easily removed from the roof to allow crane access to equipment in the building. However, the skylights also had to be strong enough to withstand Hong Kong's coastal gale force winds. Sky Roof International (Victoria) undertook the project.

Sky Roof Director, lan Howe, said the specifier's requirements and environmental concerns were met by adapting stainless steel to the company's lntalok cyclonic glazing frame system.

"The government specified that they wanted something striking, low maintenance and durable," Mr Howe said.

"As the frames had to be robust for lifting and withstand the conditions inherent in a coastal region, the obvious choice was stainless steel."

The skylight was designed to use wind uplift force to operate the lntalok hold down mechanism.

When the aluminium skylight structure is forced skyward by wind suction on the glazing, the small surface area of the stainless steel sub-frame is unaffected. This creates a differential force between the skylight and the sub-frame which is transmitted to the lntalok mechanism via the stainless steel ladders. The stronger the wind uplift on the skylight, the tighter the stainless steel lntalok engages the building.

All the prefabricated stainless steel components for the skylights were produced in a zircon glass bead blasted finish by ASSDA member Hart to Hart Fabrications (Dandenong, Victoria).

The skylights were then shipped to Hong Kong in fully fabricated kit form for easy on site assembly.

Mr Howe said ASSDA's Australian Stainless Reference Manual was vital in providing stainless steel technical and supply information.

"I found the Reference Manual and other pieces of information very useful in learning more about stainless steel and also in helping me find a fabricator for the job - Hart to Hart Fabrications," he said.

Following the success of the Hong Kong project, Sky Roof International is working on a design for a skylight featuring stainless steel glazing frames.

This article featured in Australian Stainless magazine - Issue 17, January 2001.

Tourists Supported by Stainless

Stainless steel spiral handrails provide a stunning support for climbers of Perth's new Bell Tower complex.

Grade 316 stainless steel tube was used to construct handrails for an internal spiral staircase and for an observation platform on the building's sixth floor.

170 metres of tube was used for the staircase, which was spiralled and fixed to the mild steel structure of the building. Washers and neoprene gaskets were used to separate the stainless steel from the mild steel, avoiding corrosion issues caused by dissimilar metal contact.

The handrails were fabricated by Tubelok Metals Australia in their Cannington (Western Australia) workshop and brought into the Bell Tower in six metre lengths.

Handrails on the sixth floor observation platform were secured to the structure with patch fittings through toughened glass, with 40 metres of stainless steel pipe used in total.

All handrail for the project was polished to a AWBP finish (as welded buff polished)_ Stainless steel for the project was supplied by ASSDA member Austral Wright Metals.

This article featured in Australian Stainless magazine - Issue 18, May 2001.

Style + Strength

The superior strength of stainless steel has long made it the material of choice for prison toilet facilities. Innovative styling has now opened up a new market in public restrooms. Increasingly, venues are turning to stainless steel to make their facilities safer and reduce costs in the long term. 

Vandalism in public facilities is a widespread occurrence, with some pub and club owners forced to replace a toilet every few weeks. While the initial outlay may be higher for stainless fittings, the cost of replacing and installing a ceramic pan can be recouped after just one instance of vandalism. Unbreakable stainless steel also eliminates the risk of injury from sharp ceramic shards and the inconvenience of effluent overflow.

Stylish designs mean that aesthetics aren't sacrificed for practicality. Martin O’Brien, General Manager of the recently refurbished QA Hotel in Brisbane’s Teneriffe, says stainless steel was the logical choice because it’s "tough as teeth, durable and looks good. Stainless steel was the best way to go - its clean lines never go out of date." As part of a total makeover, the QA replaced ceramic tiles and fittings with stainless steel. O’Brien says vandalism in pubs is a big issue, with "punters" taking out their frustrations in the bathrooms and causing a lot of damage to conventional fittings.

ELEGANT AND FUNCTIONAL
Metal, timber and black are the predominant themes in the $3 million refurbishment of the 120-year-old Regatta Hotel, overlooking the Brisbane River. Conceived by owner-developer Steve Hammond, the renovation juxtaposes high tech and rustic, with gleaming metal and glass surfaces set against timber frames and sandblasted brick walls. The metallic theme continues outside with stainless steel topped café tables on the pavement and verandahs, and aluminium louvres replacing traditional lattice.

Stainless steel is integral to the washroom design, combining clean, minimalist lines with durability, vandal-resistance and minimum maintenance. Push pad controls replace vulnerable taps, while moulded stainless steel pans with in-wall slimline cisterns and push pad flush eliminate other targets for vandals. Stainless steel is used for mirrors, air-towels, soap and toilet paper dispensers.

Stainless steel fabricator Stoddart, who drew on the resources of ASSDA to develop a commercial product range, says their pans are often specified as part of a suite to fit in with a high-tech, architectural look. This project used Stoddart's standard shrouded toilet made from satin finished, 316 stainless to withstand heavy duty cleaning products. A pin inside the bowl prevents objects like wine glasses being flushed into the plumbing. The flat plate design of the rim flush makes the toilet contraband-proof and the unit has the advantage of being able to be fixed onto a wall from the inside.

Stainless steel features heavily elsewhere in the bar frames and counters and in a microbrewery. Three 2 000 litre stainless steel tanks with decorative copper cladding have been incorporated into the design of the downstairs bar. The beer is piped to fermentation tanks in the upstairs bar, which form a backdrop to the dancefloor. Apart from providing a theming enhancement to a predominantly beer pub, the installation of a microbrewery was a commercial decision in response to a growing demand for boutique and specialty beers, says project manager Rob Forbes.

BEACHFRONTS AND PARKS
Local authorities present another significant market for stainless steel amenities. Gold Coast City Council, which for some years has had a policy of replacing vandalised ceramic toilets with stainless steel ones, is now installing stainless steel pans in all new public convenience blocks. To improve safety, the Council is also considering installing stainless steel woven security mesh near the entrance of public toilets. The one-way screen allows people to see if is there is a threat outside the building before exiting.

STYLISH STAINLESS SHOWERS
In conjunction with Stoddart, Gold Coast City Council is developing a prototype stainless steel shower to eliminate the corrosion problems of beachside installation. Ian Munro, Supervisor in the Council’s Building & Maintenance section, says the project has attracted interest from other councils on the coast. Seven showers are currently being tested. ASSDA member Stoddart has also manufactured stainless steel street furniture for Casuarina Beach on the Tweed Coast in northern NSW including beach-themed showers in 316 stainless. These are designed to be vandal and weather resistant and feature automatic water cut-off to prevent wastage.

Image on left: Casuarina Beach 316 stainless surfboard shower. Design by Hutton-Harris. Fabrication by Stoddart.

This article featured in Australian Stainless magazine - Issue 20, February 2002.

New Technology for Design Excellence

The overwhelming response from the architecture community to our earlier article on precision folding of stainless steel sheet using vee-cutting technology has prompted a more in-depth look at the process. 

Thanks to vee-cut technology, stainless steel sheet can be formed into angles as precise as those obtained by extrusion. This technology is now being carried out in Sydney, allowing the local manufacture of a whole range of stainless steel architectural products. The technique is particularly suited to elements such as door fronts, window frames, shopfronts, showcases, elevator doors as well as all forms of cladding.

In a completely new method of manufacture, vee-cutting can also be used to make flat products such as tread plates for lifts and escalators by removing strips of material to the required width and depth.

CLEAN LINES COMPLEMENT SPECIAL FINISHES
Ordinary bends made on a brake press typically produce a corner radius twice the thickness of the sheet, resulting in a finished product with soft, blurred lines. But with the introduction to Australia of vee-cut technology, it is now possible to produce stainless steel with corners as precise as an extruded angle, such as those found on aluminium window frames.

The method is particularly useful when working with textured and patterned stainless sheet. Such finishes are distorted by the traditional bending method. Using the vee-cut machine, the feature finish is preserved without loss of quality. This makes it the manufacturing method of choice for items such as bar fronts, display cases, door furnishings and a myriad of other uses where appearance counts.

THE VEE-CUTTING PROCESS
The machine cuts a continuous vee-shaped notch in the sheet using a series of five tools, which make repeated passes across the surface. The number of passes required varies depending on the thickness of the metal; generally three or four are needed, but up to 15 can be required for thicker product.

The machine can handle thicknesses in the range of 0.6mm to 6.0mm and is capable of cutting to a minimum depth of 0.4mm and processing sheet up to 4m in length. The sheet is then folded along the groove in a brake press. The depth of the groove can be set for acute angles down to 15°.

When used for cladding, up to 70% of the thickness of the sheet can be removed; however, care needs to be taken not to weaken structural components by removing too much of the thickness. One option is to remove material to obtain a tight corner and then stitch weld to restore strength – it is a matter of weighing up cost and other considerations.

A TYPICAL APPLICATION - ENTRANCE DOORS
An example of the finish available can be seen in the revolving doors of the McKell Building in Sydney (pictured). Byrnes Entrance Technology Pty Ltd (BET) worked with ASSDA member the Townsend Group to produce profiles and folded panel sections to clad the central steel and aluminium core of the triple door. The final effect is the appearance of a solid, triangular-shaped central column with lightly inward-curving sides.