Logo


Terrigal Boardwalk - Stainless sets the scene

The seaside town of Terrigal on the New South Wales’ Central Coast has welcomed a new addition to its foreshore with a scenic walkway using stainless steel.

The long-awaited Terrigal Boardwalk connects the existing pedestrian networks of the Terrigal Beach promenade and The Haven, providing a safe and accessible route around the headland. The new attraction provides social, health and economic benefits for the local community, allowing visitors and tourists to enjoy the public space and ocean front area.

The project was jointly funded by the Central Coast Council ($2.9M) and the NSW Government’s Restart NSW Regional Growth Environment and Tourism Fund ($2.98M). The Terrigal Boardwalk’s construction included a restoration of the adjacent rockpool, a new disability-access ramp and pathway to link the rockpool and boardwalk.

Engineered and designed by Arup, the boardwalk structure has a 50-year design life, demanding a robust design to ensure durability and longevity. The elevated boardwalk is 277m long and 3m wide, and complements the surrounding natural environment with its blackbutt timber decking and stainless steel balustrading.

The construction comprises of a reinforced concrete suspended deck structure, a suspended structural steel viewing platform with fibre-reinforced plastic open mesh, sandstone block revetment and a retaining wall ramp structure. For the bridge deck, 7.5m is the typical span of the precast deck planks between concrete headstocks on steel tubular piles. Solid concrete deck planks were chosen to protect the timber boardwalk above from wave damage and minimise overtopping for users. The boardwalk sits approximately 4.5m above sea level to be just clear of wave crests during strong weather events.

Materials selection was critical to meet the specified design life, with consideration given to the foreshore’s high level weather events and salt exposure. Grade 316L stainless steel was specified for the balustrading on both sides of the boardwalk, ramp handrailing and the rock platform staircase.

While aluminium was considered during the design phase, stainless steel was chosen due to the material’s proven performance, corrosion resistance and durability in a marine environment, and aesthetic benefits in conjunction with the timber decking and handrail specified. In addition, a costing exercise conducted by Arup presented the long-term benefits of using stainless steel outweighing its additional upfront cost over aluminium.

Constructed by Land and Marine Group, the project involved a high level of collaboration between multiple local suppliers and service providers to meet the exacting demands of the specification. 

ASSDA Member Synergy Engineering was engaged to fabricate and install the stainless steel handrails, balustrades and stairs, spotted gum timber railing and the structural steel viewing platform. The project involved the stainless steel fabrication of 247 balustrade panels, 119m of handrail balustrade and an 8-step 1200mm wide staircase with fibre-reinforced treads. TIG welding techniques were used throughout the fabrication and installation process to ensure precision and a clean aesthetic.

ASSDA Member Atlas Steels supplied over 15t of 316L stainless steel, including 3402m of 30x8mm flat bar and 1656m of 70x10mm flat bar. The project was undertaken in the midst of the COVID pandemic, presenting a number of challenges with the supply of imported stainless steel material and shipping lead delays. As a result, Atlas Steels took the initiative to laser cut stainless steel plate to size and engaged ASSDA Member Decoware Australia to polish the material to specification. Starting with a coarse 80 grit through to a 400 grit finish, a surface finish of Ra <0.5 µm was achieved. The resourcefulness of local service and skill assisted in meeting the project program, delivering a resolution for the unprecedented challenges.

A small proportion of material was sourced from ASSDA Member Viraj Profiles, and ASSDA Member Vulcan Stainless supplied an additional 11t of laser cut 5mm, 10mm, 16mm and 20mm 316L stainless steel plate for the project.

Following fabrication, all stainless steel balustrade panels and handrails were electropolished by ASSDA Member Australian Pickling & Passivation Service and delivered directly to site for installation by the Synergy Engineering team.

The beautiful coastal boardwalk features a viewing platform, integrated seating, LED lighting and access to the rock platform. Offering uninterrupted views of the Pacific Ocean and beyond, the Terrigal Boardwalk is certain to meet the performance requirements of its design with its quality construction and use of stainless steel. 

The Terrigal Boardwalk officially opened on 14 April 2021, with its first steps taken by local crowds alongside the New South Wales Premier Gladys Berejiklian, Parliamentary Secretary for the Central Coast, Adam Crouch, Central Coast Council Administrator, Dick Persson, and the Council’s new CEO, David Farmer.
 
    

This article is featured in Australian Stainless Magazine issue 72, 2021.

Structural design of stainless steel

Stainless steel is used for a wide range of structural applications including:

  • Beams, columns, platforms and supports in processing plant for the water treatment, pulp and paper, nuclear, biomass, chemical, pharmaceutical, and food and beverage industries;

  • Primary beams and columns, pins, barriers, railings, cable sheathing and expansion joints in bridges;

  • Entrance structures, canopies, cladding and support systems for masonry;

  • Security barriers, blast walls, hand railing and coastal structures. 

Case studies of a range of structural applications are available at the case studies section of  www.teamstainless.org/resources/information-center-for-stainless-steel-in-construction.

This introduction to structural design in stainless steel aims to highlight differences between the material properties and structural behaviour of stainless steel and conventional carbon steel normally used for structural purposes, e.g. grade 350 to AS 3678 and AS 3679.

It should be noted that stainless steel structures should not be simply designed using design standards for carbon steel, such as AS 4100 and AS 4600, because of the significant differences between the mechanical properties of carbon and stainless steels.

Selection of an appropriate alloy of stainless steel is the first step in any design process.

Austenitic stainless steels are most widely used for structural applications, though the use of duplex stainless steels is increasing, where it is possible to exploit the benefit of high strength (around 460 MPa, compared to a strength of around 220 MPa for austenitic stainless steels). This can be particularly valuable in weight-sensitive structures like bridges or on offshore topsides. Duplex stainless steels are more likely to be used in heavier gauges. Ferritic stainless steels are also suitable for structural applications, offering a corrosion resistant alternative to many light gauge galvanised steel applications. They are generally used in gauges of 4 mm and below although the 12% chromium utility alloys are used in thicker sections (vehicle chassis or high temperature ducting) when minor rust staining can be allowed.

Material properties

From a structural viewpoint, the main property that distinguishes stainless steel from carbon steel is the stress-strain response. In contrast to carbon steel, for which the stress-strain curve may be modelled as bi-linear for most compression and flexural member design purposes, the stress-strain curve of stainless steel is generally highly non-linear and without a distinct yield point. Figure 1 compares the stress-strain characteristics of various stainless steels with carbon steel for strains up to 0.75% and Figure 2 shows typical stress-strain curves to failure. (The figures show stress-strain curves which are representative of the range of material likely to be supplied and must not be used in design.) The distinctive mechanical properties - considerable strain-hardening and ductility - make austenitic and duplex stainless steel particularly well suited for structures required to withstand accidental loading due to their high energy absorption characteristics.

In the absence of a clear yield stress, it is common practice to define an equivalent yield stress for stainless steel by using a proof stress, usually the 0.2% proof stress. (By definition, the plastic - or permanent - strain at 0.2% proof stress is 0.2%.) The proportional (or linear) limit of stainless steels’ deflection ranges from 40 to 70% of the 0.2% proof stress.

As a result of the non-linearity, stainless steel loses stiffness at low stress levels. This affects the design rules for members that rely on stiffness to transfer loads, notably compression members and unbraced flexural members.As well as nonlinearity, the stress-strain characteristics of stainless steel also display non-symmetry between tensile and compressive behavior and anisotropy, i.e. differences in behaviour of coupons aligned parallel and transverse to the rolling direction. In general, anisotropy and non-symmetry increase with cold work and so are more significant in the design of lighter gauge heavily worked sections, rather than thicker walled structural sections.

It is possible to enhance the strength of austenitic stainless steel by cold-working to a much greater extent than for carbon steel.

The initial modulus of elasticity (Eo) of stainless steel alloys is slightly lower than that of carbon steel.

The behaviour of stainless steel at elevated temperatures differs to that of carbon steel because of the metallurgical differences caused by the composition. Stainless steel retains a greater proportion of its strength at temperatures above about 550 °C and shows better stiffness retention at all temperatures, which is important in design against fire for components such as blast and fire walls.

The coefficients of expansion (CTE) of austenitic stainless steel alloys are larger than those of carbon steel. At the same time, the thermal conductivity is lower. While the CTE is important in determining thermally  induced stresses and deformations, the combination of larger coefficient of expansion and lower thermal conductivity has the effect of substantially increasing the risk and possible extent of welding distortions than those experienced in fabricating carbon steel structural member. The duplex grades have similar thermal conductivity to the austenitics but with 20% lower CTE so the risk of welding distortion is slightly lower than with austenitics. 

Specifications and reference documents for design of  stainless steel structures

American Society of Civil Engineers (ASCE) has revised ASCE 8 Specification for the design of cold-formed stainless steel, applicable to lighter gauge austenitic and ferritic material in the annealed and temper-rolled condition (Reference 1). The 2002 version has been substantially updated because of extensive research work and will be issued late in 2021. This includes alternative treatments of compressive loading, i.e. effective width and direct strength. The structure of AISC 8 will be familiar to those using AS/NZS 4673:2001 although 4673 has now been withdrawn as an aged standard.

Also in 2021, the American Institute of Steel Construction (AISC) will release a new standard (reference 2) AISC 370 Specification for Structural Stainless Steel Buildings to reflect the substantial increase in the use of heavy structural stainless steel sections. It includes hollow sections as well as welded, hot rolled and bar products. It will be accompanied by AISC 313 Code of Standard Practice for Structural Stainless Steel Buildings (Reference 3) and an updated 2nd Edition of the 2013 AISC Design Guide 27: Structural Stainless Steel.

The Eurocode for stainless steel design, EN 1993-1-4, covers welded, hot rolled and cold formed products made from austenitic, duplex and ferritic alloys, at room temperature and in fire (Reference 4). The Design Manual for Structural Stainless Steel (4th Edition) was published in 2017 and gives essential information needed by designers concerning alloy selection, durability, material properties, design rules and fabrication, in accordance with EN 1993-1-4 and other European standards (Reference 5). A Commentary explains how the design expressions in the Recommendations were derived and gives background information and references. Design Examples demonstrate the use of the Recommendations. Section property and member capacity software is also available, all aligned to EN 1993-1-4.

This Design Manual and these supporting design tools are freely downloadable from www.steel-stainless.org/designmanual.

This article has been extracted from the 2020 Australian Stainless Reference Manual, available for purchase at assda.asn.au

REFERENCES: 1. ASCE 8-02 Specification for the Design of Cold-Formed Stainless Steel Structural Members, SEI-ASCE 8-02.  \   2. AISC 370-2021  \   3. AISC 313-2021  \  4. EN 1993-1-4:2006+A1:2015 Eurocode 3. Design of steel structures. General rules. Supplementary rules for stainless steels.  \   5.  Design Manual for Structural Stainless Steel, SCI Pubilcation P413, The Steel Construction Institute, 2017 (available from www.steel-stainless.org/designmanual).



This article is featured in Australian Stainless Magazine issue 72, 2021.

Lighting up Chinatown

Stainless steel lanterns now adorn the streets of Melbourne’s Chinatown, celebrating the cultural character of the longest continuous Chinese settlement in the western world.

Chinese lanterns are a symbol of Chinese culture worldwide, initially used to provide light and later adopted for religious worship, decoration and celebration. Traditionally made from silk or paper, the City of Melbourne recently evolved the Chinese hanging lanterns featured on Little Bourke Street from cloth to stainless steel.

In extensive consultation with the Chinatown Precinct Association, the City of Melbourne and GHD (Structural Engineers) reimagined the classic lantern with a detailed design that preserved the traditional aesthetic while examining a number of considerations. 

Durability and product life cycle were strong factors to reduce maintenance and regular replacement of the lanterns. Strength-to-weight ratio and resilience to local weather conditions was also important, with the completed design required to stay below 7kg to be viable for use on the existing catenary lighting system.

ASSDA Member Draffin Street Furniture worked closely with the City of Melbourne to bring the design to life, assisting with the materials selection and manufacturability of the lanterns. Two prototype lanterns were installed at the corner of Heffernan Lane and Little Bourke Street to test the design and seek feedback from local traders and the Chinatown Precinct Association.

Powder coated aluminium was initially selected as the design material however, stainless steel superseded the specification primarily for its strength and the ability for a thinner section of material to be used (0.6mm stainless steel sheet vs. 1.22mm aluminium sheet). In addition, stainless steel offered a more sustainable solution with a 25-year design life and little-to-no maintenance.

The final design resulted in a 700mm wide by 500mm high spherical lantern made from 316 grade stainless steel, powder coated with a luminous, metallic red colour. In Chinese culture, the colour red symbolises good fortune and joy. 

The lanterns were formed using laser cut 0.6mm sheet, with each panel formed into shape and fixed to a central aluminium frame. The custom-designed lanterns were manufactured by Draffin Street Furniture, and stainless steel material for the project was supplied by ASSDA Member Steel Color Australia.

80 new permanent lanterns were installed on the existing catenary lighting system, which was originally manufactured and supplied with the assistance of ASSDA Member Ronstan Tensile Architecture in 2009. The linear grid catenary suspended from the street’s buildings uses 316 grade stainless steel rectangular frames spaced equidistantly to hold the grid form, while permitting the suspension cables to connect to buildings at different heights depending on the availability of structural connection points. Designed to enhance the character of the precinct with Chinese lanterns and other iconography, the decorative and functional stainless steel catenary lighting system continues to perform structurally 12 years on since its installation.

Installation of the new hanging lanterns was completed at the end of July 2020. Brought to life using local design expertise and stainless steel, the lanterns maintain its symbolic heritage and will continue to provide a festive welcome to visitors for at least the next 25 years.
       

Image: @rayofmelbourne for @cityofmelbourne

This article is featured in Australian Stainless Magazine issue 72, 2021.

Stainless steel ignites  luxury, style and warmth

ASSDA Member and Accredited Fabricator Southern Stainless have taken outdoor entertaining to a new level with their custom-designed and Australian made stainless steel gas fire pit.

Alfresco living is a strong part of Australian culture, and Gold Coast based Southern Stainless saw an opportunity to bring warmth and elegance to the outdoor space with the use of stainless steel. Starting the design process in 2015 and with over 18 months of research and development, a stainless steel gas fire pit was born, meeting both Australian Standards and gas regulations. 

Elegant and simplistic in its design, Australia’s harsh coastal conditions inspired the firepit’s construction. Grade 316 stainless steel sheet with a 2B finish is used to construct the sleek body, door and burner tray, and 1.5mm 316 stainless steel tube is used to assemble the burner and legs. The fire pit has a stainless steel burner mounted into an enclosure to accommodate toughened glass pebbles surrounded by safety glass. Gas filters through the pebbles and ignites fire, giving the appearance of a floating flame.

Southern Stainless’ fire pits are available in square and round models, and measure 1m x 1m or 1m diameter. Both are fitted with two flame failure devices that automatically shuts off the gas if the primary pilot blows out. The flame failure devices provide additional safety while also making the fire pit extremely effective in windy conditions.

The fire pits have an LPG bottle compartment or can be designed to be plumbed into gas. In both instances, the fire pit comes with the gas controls and burner fully assembled. Only the glass safety sides need to be installed along with the toughened glass pebbles. If configured to be plumbed into natural or LPG gas, the appliance can easily be connected by any qualified gas plumber, or if ordered with an LPG bottle compartment, no installation is required.

Stainless steel is the clear material of choice when considering the great Australian outdoors. Grade 316 stainless steel has excellent corrosion resistance properties with an increased ability to resist pitting and crevice corrosion in warm chloride environments when compared with grade 304. It resists rusting in virtually all architectural applications, and is a durable, heat resistant and aesthetically appealing material option.

Stainless steel fire pits are built-to-last and combine physical warmth with visual luxury, offering year-round ambience to cater for the way of Australian outdoor living.


 

This article is featured in Australian Stainless Magazine issue 72, 2021.

 

A new twist on stainless design

With a striking and innovative design evoking visions of the Singapore based Helix Bridge, stainless steel has formed an integral part in creating one of Sydney’s most exciting new structures.

Commissioned by Landcom as part of the Lachlan Line Precinct development project in North West Sydney’s Macquarie Park, the yet to be officially named cyclist bridge provides visual flair, safe accessibility, and excitement to the area. In an area with typically heavy traffic congestion, the project’s promotion of reduced car dependency creates a significant positive impact to the surrounding environment.

The design is the first of its kind in Australia, utilising a double helix arrangement with a varying diameter along its curving 178m length. While the design elements certainly lend themselves well to aesthetics, structural requirements dictated much of the overall shape. A steel truss arrangement is used, required for the long sections spanning the multiple roads below its footprint. The diameter of the spiral increases at the bridge supports and tapers along its span.  At its narrowest, it is 5.5m in diameter, and 7.8m at its widest.

Approximately 170t of 2205 grade duplex stainless steel was used, along with around 220t of structural mild steel. Due to the large quantity of material required, multiple distributors supplied material mostly on an indent basis, with some delivered ex-stock. ASSDA Members Midway Metals, Stirlings Performance Steels and Vulcan Stainless all supplied material, with the majority of plate (up to 80mm in thickness) produced by ASSDA Member Outokumpu, managed through their Melbourne office. 

A minimum 100-year service life with minimal maintenance (becoming increasingly common in the design of bridges) was a key criterion, particularly important for the hard to access structural components. From the beginning, 2205 duplex grade presented as an ideal material, thanks to its hybridised microstructural properties granting it superior mechanical properties to many forms of mild and stainless steel. 

Put simply, being stronger allows for thinner sections to be used or, alternatively, more scope for efficient design such as larger spanning or increased resistance to bending moments. Mild steel was retained  for the helical outer structure, and painted blue, which was a central design requirement. 

Arup proposed duplex stainless steel for the deck structure and wearing surface within the helix due its increased strength to weight  properties whilst maintaining high durability performance.   

Outokumpu played an instrumental role in advocating the use of the material properties of duplex grade at the early design and concept stages. Backed up by global materials experts and with a wealth of expertise in supplying stainless materials for bridges all over the world, Outokumpu aimed to provide a technical solution through the use of duplex stainless, rather than simply tender for the supply of material. “The use of duplex stainless steels in bridges around the world is becoming more and more the material of choice, so it was great to see Arup in Australia embrace it in its design”, said Con Logos, Vice President APAC at Outokumpu. “A special thanks to George Miech from my team for his tireless effort in the early stages, working closely with both Arup and RMS to have duplex stainless specified”. 

Outokumpu also assisted the fabricator and the end client, Transport for NSW, with expertise, advice, and preliminary procedures in welding the material, particularly vital with the thicker sections which require great care to ensure optimal material properties are realised in the weld and adjacent areas.

The bridge was fabricated in Sydney in four modules, which were trial assembled prior to being delivered to site, where the four segments were positioned and secured over the course of four weekends. Specially designed lifting assemblies were necessary to ensure the segments were not overstressed. 

As bridge design increasingly demands greater durability, aesthetic and creative licence and structural performance, stainless steel, of the duplex family in particular, presents a wonderful option now and into the future.

Photo credit: Landcom

This article is featured in Australian Stainless Magazine issue 71, 2021.

 

Comparisons of hot and cold formed stainless steel

When comparing hot and cold formed stainless steel, the first question you would ask yourself is: are there any chemical differences between the two? ASSDA has previously published articles on the various surface finishes including the few hot and multiple cold finished processes, however this article concentrates on the differences. 

Since the 1970s, most stainless steel is produced by melting in an Electric Arc Furnace (EAF) and then the molten stainless steel is transferred to an Argon Oxygen Decarburisation (AOD) vessel or, less commonly, a Vacuum Oxygen Decarburisation (VOD) vessel. These processes control impurities such as carbon, sulphur, nitrogen, hydrogen and other impurities which could form oxide precipitates. For critical applications such as aerospace or precipitation hardening alloys, further refining is possible, but this is a smaller market. Critically, in AOD, using the injection of inert argon as the stirring agent into the melt allows control of nitrogen additions, e.g., for duplex or high austenitic stainless steels.  

Chemistry

The basic chemistry of a specific grade of stainless steel is the same regardless of how it is subsequently shaped, i.e., as hot or cold rolled, hot forged, cold drawn/shaped or simply cast –  with the proviso that cast stainless steels typically have more chromium and (often) more silicon than their wrought counterparts. In addition, even if cast products have been stress relieved, their microstructure is dendritic so that there can be significant composition differences (localised differences in corrosion susceptibility) between the early solidifying dendrites and the final bulk solidification.

Hot formed

Producing hot formed stainless steel is deceptively simple as shown in the graphic. Currently, for about 95% of production, the molten metal is decanted from the AOD into a cooled continuous caster and emerges horizontally as a slab. The microstructure in the slab is columnar from the outsides (because of the cooling by the caster walls) with a relatively uniform equaxial microstructure in the centre. It is also covered with heavy black oxide scale with a chromium deficient layer underneath – as with weld tints. Typically, the slab is then surface ground to remove solidification features and the scale which would both otherwise be incorporated into the surface during subsequent rolling. The slab is then charged into a reheating furnace and hot rolled to homogenise the microstructure and provide either plate or coil as the product form. The grains will now be more oriented along the rolling direction. The microstructure is then further refined (and internal stresses reduced) by annealing above 1000oC.

Unless the steel is to be used where appearance and maximum corrosion resistance is not critical, e.g., in a furnace, then after hot rolling it would be shot blasted to break up the scale and then pickled. The pickling causes the dimpled appearance of a Hot Rolled Annealed and Pickled (HRAP) plate surface because the pickling acid attacks the base metal at the defects in the black oxide scale. It also gives a typical surface roughness of 5 or 6 µm Ra. There is a potentially cosmetic corrosion issue if the (typically) fast pickle does not completely remove any shallow intergranular oxide penetrations, however this is unusual. For long product such as angles or channels, another visual distinction is that the edges meet at 90o compared to the radius of curvature determined by the thickness and ductility of a cold rolled product.

Cold formed

Cold rolled flat product is quite different because it usually starts at room temperature with a dimpled surface and finishes with thinner material – and watching the increase in speed of the sheet as it gets thinner is quite startling. There is a significantly more elongated microstructure along the rolling direction, and this enhances the anisotropy in transverse to longitudinal strength compared to the relatively slight effect for hot rolled material. Long product is not cold rolled but more correctly it is cold  shaped or formed.

The increase in strength with cold work can be substantial, especially in thin materials as the cold work increase can enhance the strength of the full depth. As an example, the table from ASTM A666 data shows the substantial change in mechanical properties for 304 from annealed to half hard, i.e. half the absolute maximum possible strength – which would have negligible ductility.

Effect of cold work on strength and ductility of 304

One effect of the increase in strength with cold work is that the limit of proportionality will increase with cold work, i.e., the linear deflection occurs up to a higher stress. The reduction in break elongation is simply reflecting the proof stress closing on the tensile stress from 40% to 73% as shown below.

Variation of thickness tolerances for cold and hot rolled materials

There are also differences in the tolerance between cold and hot formed material as shown by comparisons in A480 (flat product – sheet vs. plate) and A484 (sections). However, it is not as simple as “hot formed is less precise than cold formed” as seen below. 

Surface finish

Often it is important to consider appearance and corrosion resistance to the “bright and shiny” benchmark. Hot rolled material is always going to be dimpled, even when it is electropolished and exhibiting a brilliant lustre. It will be marginally more difficult to clean than a smoother cold rolled surface but abrading the surface to give a roughness of less than 0.5 µm Ra is counterproductive. You lose the passive stainless steel and an abraded surface potentially has sulphide inclusions exposed compared to the original pickled, sulphide free HRAP surface.

The inherent roughness of a cold rolled sheet decreases steadily as the plate is rolled thinner as shown in graph. It shows the decrease of Ra from the crushing of the peaks left from the hot rolling as the sheet gets thinner. The graph is for cold rolled annealed and pickled (2B) material and is useful when someone asks for a 2B finish for a thickness not in the band. However, thickness of pickled materials is not relevant to the corrosion resistance whereas the Ra is critical to an abraded surface both for reasons of cleanability and possible crevices from torn surface flaps plus, if not passivated, exposing sulphide inclusions.

 

This article is featured in Australian Stainless Magazine issue 71, 2021.

 

Award-winning stainless food plant

World-class processing systems demand high quality products, innovative features, and long-term yield increase, all of which have been delivered through superior workmanship, engineering, and the use of stainless steel.

ASSDA Member, INOX Australia, was engaged by a Melbourne based stock and soup manufacturer to design the integral process, fabricate, install, and commission a beef, chicken, seafood, and vegetable stock processing system. The processing system is entirely fabricated in stainless steel as it has been essential to the project design and fabrication, being the material of choice in demanding hygienic environments that involve high heat. 

Exceeding their client’s expectations, INOX supplied a processing system that provided multiple innovative features, winning the 2019 Food & Beverage Industry ‘Innovative Technology of the Year’ Award, and being nominated for ASSDA’s 2019 Fabricator Project of the Year Award. This extraordinary processing system features a single user operational interface, safe and ergonomic handling of the product during the process from start to finish and hygienic design of the process including zero wastage at end of production. It also improved the yield of raw materials by pressure processing instead of traditional atmospheric process.

The system works by depositing 1000kg of raw materials into a stainless steel basket which is lifted by an electric hoist into the automatically opened pressure vessel. The touchscreen operational interface is used to set and supply the water volume. The process is fully automatic to the set parameters and then alarms when the process is completed. Following the cooking procedure, the CIP (Clean In Place) water is circulated through the heating jacket of the vessel which serves two purposes. The first is to cool the cooking vessel to a temperature that allows the product to be discharged, and the second, to use the heat recovered from the cooking vessel to heat up the cleaning water. This reusable use of heating allows for no external heating of the cleaning water.

The liquid stock produced is then pumped through a specially designed filtration system, to a holding tank which is then ready for the product to be received by the external filling line. The stainless steel basket is then removed from the vessel and the waste product is dumped into a hopper underneath the basket, ready to be removed to a disposable waste bin. The basket is then cleaned within the vessel during the CIP process and does not exit the food processing room at any point, ensuring the equipment is cleaned and cannot be contaminated externally. 

An impressive 5000kg of 304 and 316L grade stainless steel was used to complete the project. All stainless steel material was supplied by ASSDA Members, Midway Metals, Vulcan Stainless and Tubesales Stainless. This included stainless steel tube, pipe, plate and sheet with 3mm to 12mm thickness. Several components (with thicknesses up to 75mm) required a large amount of specialised machining. The material was mechanically polished where required to achieve a better than 0.8 µm Ra surface finish. This superior material of choice meets the project’s sanitary requirements, offers structural integrity and excellent corrosion resistance in high temperature applications. 

 

This article is featured in Australian Stainless Magazine issue 71, 2021.

 

Stainless steel – a mainstay in water assets

A mainstay in the processing of sewage water in water recycling applications, stainless steel once again plays a critical part in working towards a sustainable future.

Western Water Treatment Plant (WWTP), south of Werribee in Melbourne’s Western District, is a critical asset responsible for processing around half of the city’s total sewage. The process requires a massive footprint, where a series of large lagoons use anaerobic (without oxygen) and aerobic (with oxygen) bacteria to sequentially break down and clean the feed water of solids and gases. The resultant recycled water is used for multiple non-drinking purposes, including irrigation and firefighting. 

WWTP is also largely energy self-sufficient. This energy is captured during the sewage treatment process by combusting biogas, which is captured under the covers. Biogas is used to meet much of the Plant’s electricity needs – preventing hundreds of thousands of tonnes of carbon dioxide entering the atmosphere each year. 

The site carries significant environmental importance to both the immediate and wider areas. Biogas production from the process is used to meet all the Plant’s energy needs through on-site power generation. The Plant is an enormous site – almost the same size as Phillip Island and a world-renowned wetland, declared a Ramsar site in 1983. It is home to many species of flora and fauna and a haven for birdwatchers – in summer it can host more than 100,000 birds in a month.

With current capacity concerns in the existing plant network, stretching back 120 years, and a forecasted increase in processing demands due to a growing city, the need for an additional nutrient removal plant (to complement the existing two) was established. More efficient in design and with more advanced monitoring and controls to provide class A recycled water, the new plant provides an additional 140ML of treated water per day. The plant was designed by Jacobs and built by UGL and CBP Contractors, with commissioning in 2019.

Grade 316L stainless steel was selected as a default material for the pipework, in 2B finish. Offering strong corrosion resistance even against contaminated effluent water, its ease of fabrication and ability to be installed without the need for coating and subsequent maintenance was also important.

ASSDA Member and Accredited Fabricator Roladuct Spiral Tubing was selected to manufacture and supply approximately 50t of spiral welded large diameter pipe, ranging from 300 to 1422mm in diameter. Feed material was supplied  by ASSDA Member, Midway Metals to Roladuct’s  Melbourne manufacturing site. 

Roladuct was nominated in 2019 for the ASSDA Fabricator Project of the Year Award, with judges impressed by the quantity of stainless steel used, as well as the significant environmental benefits realised by the plant upgrade.

As water assets continue to be upgraded and optimised for a growing country, stainless steel will continue to play a vital role in providing material performance and plant reliability for years to come.

 

 Photo credit: Roladuct Spiral Tubing

This article is featured in Australian Stainless Magazine issue 71, 2021.

 

Screening Melbourne’s drinking water

Stainless steel is playing a vital role in delivering effective bulk water intake screens for Melbourne’s water supply.

Designed and manufactured in Brisbane, ASSDA Member Aqseptence Group Australia has recently delivered one of the largest passive intake screens in the Southern Hemisphere. Having produced more than 4,000 screens for the last  50 years, this latest milestone achieved a nomination in the hotly contested Process Industries category of the 2019 ASSDA Fabricator Project of the Year Award. 

In mid-August 2019, Aqseptence Group was engaged by a joint venture of John Holland and KBR to provide design and construct services for a significant capital works project, covering multiple Melbourne Water assets. The screen is used as a bulk water transfer screen for the O’Shannassy Dam, located east of Melbourne. Distributing clean drinking water  to most parts of Melbourne, it is a critical asset storing  3.1 gigalitres of water among a series of reservoirs on the city’s periphery. The mammoth screen took  approximately two months to design and manufacture.

The Johnson Screens T96E passive intake measures an impressive 8.6 metres wide and stands 3.6 metres high.  It is constructed entirely in grade 316L with a mill finished  plate and No. 4 finish wedge-wire and bar. K-Tig welding  was used to join 10mm plates to achieve overall plate size  to roll into tubes. The entire fabrication was then pickled  and passivated. Grade 316L, a standard material of construction at Aqseptence Group, was specified for the grade’s ability to resist general and localised forms of corrosion, a risk even with relatively low chloride inland  water sources. Additionally, being easy to source and  fabricate, its versatility in taking many forms and profiles  is clearly on display.

The intake screen is used to provide an uninterrupted water withdrawal source while protecting assets from foreign matter and most importantly, protecting wildlife by guaranteeing uniform and low through-flow velocities. This fish-friendly screen is also a passive design as it has no moving parts, therefore simplifying maintenance and reliability. Aqseptence Group’s Vee-Wire slot system was used to ensure uniform flow through the screen at a controlled velocity, to protect surrounding marine life. Additionally, using the strength properties of 316L, the screen has sufficient mechanical rigidity to support its own weight along with hydrostatic pressures. Stainless steel was specified due to its low impact on the environment, on both the reservoir and the clean drinking water it supplies, paired with its durability, corrosion  resistance and material strength attributes.

Aqseptence Group is now focused on working with the broader network of water infrastructure authorities to help upgrade their water supply assets and continue to service  the City of Melbourne for future generations with the use of stainless steel.

This article is featured in Australian Stainless Magazine issue 70, 2020.

 

Seven ways to prevent tea staining of stainless steel

When used properly, stainless steel enjoys a strong and enduring reputation for visual appeal and structural integrity in a wide range of applications and environments. But, like all materials, stainless steel may become stained or discoloured over time, impairing the overall look. This brown discolouration - tea staining - has been identified in coastal applications in Australia and overseas.

In the late 1990s, the newly formed ASSDA Technical Committee researched the reasons for the brown discolouration. ASSDA’s work, in collaboration with the International Molybdenum Association, led to guidelines published in 2001 explaining the causes and remedial techniques. The work was later refined to ASSDA’s FAQ 6. This clarified some of the misunderstandings that have circulated about atmospheric exposure and possible corrosion of stainless steels. It does not deal with immersed exposures.

Corrosive chemicals in the atmosphere

In a clean atmosphere, the relative humidity is sufficient to maintain the thin self-repairing passive film which protects stainless steel. Given that chlorides are known to cause corrosion, locations within line of sight of the sea will tend to corrode, especially with onshore prevailing winds. 

Extensive research using corrosion coupons has classified corrosivity using carbon steel and zinc while measuring corrosives such as chloride and sulphur dioxide – as an indicator of industrial activity. AS 4312 presents maps with bands of corrosion rates (from extreme to low) and corrosion rates with distance from the sea or a bay.  For sheltered waters, corrosion rates drop to medium or lower within a few hundred metres, while for exposed areas like Cape Leeuwin in WA, Newcastle in NSW, or Cape Jervis in SA the rates can remain extreme to high for kilometres inland.  

The AS 2699 series of standards for ties used for brick fixing in walls uses deposited chloride measurements to arrive at similar bands of corrosivity. Those values define zones where increasing thickness of galvanizing or, 304 or 316 must be used successively depending on distance from the sea to achieve the design life in buildings. In rural or urban environments, corrosion of stainless steel is unusual although cosmetic staining can occur from vegetation, chemical spills or blown dust.  

Atmospheric conditions

Stainless steel will not corrode unless there is a sufficient concentration of aggressive ions (generally chlorides) and there is free water but not a sufficient flow to wash away contaminants. Water will condense on clean metal if the temperature falls below the dewpoint  but if there are chloride salts, then there is a lower critical relative humidity (RHcrit) which will form an aggressive salt solution by absorbing moisture from the air. This means that deposited sea salt can cause corrosion although the temperature is still below the dewpoint for a  clean surface.  

A secondary atmospheric factor is that corrosion rates roughly double for every 10oC rise in temperature; all else being equal. For instance, corrosion staining will be worse in Darwin than in Hobart.

Design, cleanability and drainage 

Open, bold exposures allow natural rainfall to wash away grime and potentially corrosive deposits. However, drying retained runoff on horizontal surfaces, surface tension at sharp edges, in crevices, or in horizontal abrasion lines on vertical surfaces, all cause increasing corrosivity and do not meet the “bright and shiny” expectations for stainless steel.

Surface roughness and standards

The widely publicised surface roughness of “no more than 0.5µm Ra” for a tea staining resistant surface is codified as 2K in EN 10088.2 which includes a requirement for a clean cut profile, i.e. no flaps or sharp edges. ASTM A240/A480 suggests that a good fabricator can achieve about 0.6µm Ra for a No. 4 finish.  ASSDA conservatively recommended finishing with 320 grit for 0.5µm. Ra is readily measured mechanically or by laser reflectance but, because multiple surface profiles can give the same Ra value, samples are frequently used for acceptance tests. Rough surfaces show significant tea staining.

Unfortunately, the 0.5µm Ra requirement is sometimes specified for HRAP plate with a typical finish of Ra ~6µm. This causes un-needed expense in removing metal. Both thick HRAP plate and thin 2B (or BA) sheet or coil were pickled as their last processing step. Even with Ra greater than 0.5µm these finishes have good resistance to tea staining. However, a rougher surface is still less cleanable and is generally not as bright. Smooth 2B or BA finished sheet has good resistance to tea staining.

There is ample evidence that smoother surfaces resist corrosion better and a mirror polish is the best possible mechanical finish. ASTM A240 and EN 10088.2 have descriptive definitions (for No. 8 or 2P respectively) which centre around high reflectivity and image clarity but do not specify Ra.

Electropolishing electrochemically cleans the surface, removes sharp edges and smooths microroughness. It provides a deep lustre but not necessarily a clear reflection. However, it only slightly reduces Ra, e.g. 0.7 to 0.5 µm for a linished strip. Electropolished surfaces have excellent resistance to tea staining.

Chemical cleanliness of the exposed surfaces

Stainless, carbon or galvanised steels may be fabricated in adjacent areas and carbon steel can contaminate the stainless steel either as floating grit or if tooling is used on stainless steel after processing carbon steel. Contamination during transport or handling is also possible. Any moisture will immediately corrode the carbon steel and cause a large brown stain compared to the contaminating particle - this is not tea staining. The illustration shows a rooster tail of carbon steel contamination on a stainless steel surface from cutting Colorbond® nearby. The contamination can be removed by pickling or, more slowly, by a passivating nitric acid application. The widespread pale spots are light tea staining.

In addition, an oxidising passivation treatment after the final metal removal substantially improves corrosion resistance, partly because the final passive film is thicker and has a higher chromium to iron ratio. However, for freshly abraded surfaces, the sulphide inclusions inherent in all steels are initiation sites for corrosion unless they are removed by a passivating acid. Bar product has more inclusions with at least 10 times the sulphur content of sheet or plate to aid machining. Nitric passivation does not change the appearance of even a mirror polished surface but does significantly increase its corrosion resistance. Further details of pickling and passivation are given in ASTM A380.

What alloy should be selected

An ASSDA/IMOA selection tool is available by searching for ‘stainless-steel-selection-system’ on www.imoa.info. It asks about environment, finish, orientation and maintenance before providing a recommended material from 304 for urban or rural exposures up to 2205 for severe marine. It does not include ferritics mainly because they are not as widely used in welded fabrications. Alloys with similar or higher corrosion resistance (as assessed by PRE) could be substituted. Super alloys are not usual for atmospheric exposures.

Maintenance – natural and/or applied

Stainless steel is low maintenance but not no maintenance. A rule of thumb is that if an adjacent window (or glass screen) needs washing, wash the stainless steel. FAQ 6 has recommendations including consideration of retained deposits and rain washing. One sub-tropical beachside council has implemented a 3 to 4-month cycle of a high pressure wash with low chloride water and detergent (and possibly a zero chloride solvent) before a fresh water rinse. Domestic cleaners, even non-abrasive ones, are not recommended as some have chloride activators and, because of their hygiene image, may have some bleach - which are both potentially detrimental.

This article is featured in Australian Stainless Magazine issue 70, 2020.

 

Stainless steel - The right choice for an environmentally sustainable upgrade

Stainless steel provides a cutting edge and environmentally friendly solution for industrial applications.

Dow Chemicals, a global chemicals manufacturer, recently completed a major upgrade of the wastewater treatment system at their Victorian Point Henry coatings plant. The plant manufactures acrylic emulsions which find use in numerous applications including house paints. ASSDA Members Stirlings Performance Steels and Barwon Valley Stainless provided supply and fabrication services for this impressive wastewater treatment facility upgrade. 

Wastewater produced in the production facility is pumped into flocculation tanks for settling and the clear supernatant is sent for further biological treatment. This treated water is recycled back to production but is also used for irrigation on site to minimise freshwater consumption.

Geelong based Barwon Valley Stainless is a preferred Dow contractor and was selected to provide the complete scope of services for the wastewater treatment plant upgrade due to their knowledge and expertise of wastewater treatments, both local and interstate. Their quality workmanship was reflected in this project as they provided civil and structural works, tank and pipe spooling fabrication, site installation and pump station commissioning. With over 25 years’ experience and competence in stainless fabrication, they were able to work successfully within Dow’s project time and location constraints. 

Stirlings Performance Steels supplied the entire portfolio of materials to Barwon Valley Stainless. This included cut-to-length large bore pipe, structural rectangular hollow section and various pipe fittings as well as laser/plasma profiled plate which were all in grade 316/L.

Reducing environmental footprint in industrial applications is important and material selection is a critical step in both maximising the lifetime of plant and equipment, while minimising the need for maintenance and servicing. This upgrade successfully satisfied both these requirements with the use of stainless steel. Grade 316 is a popular material of construction where water is processed with relatively low chlorides at ambient temperature. It provides an optimal cost benefit compared with other steel-based alternatives which require coating or lining. Additionally, the close proximity of the site to Victoria’s Corio Bay requires resistance to corrosion from airborne seawater. According to Ben Arlidge, Project Manager at Dow, “Stainless steel has provided the perfect mix of performance, workability and cost for our new wastewater treatment facility.”

The plant upgrade is a major step in providing long term certainty to the local Moolap economy, as well as in strengthening the Australian supply chain of domestic market paint products. 

 

Photo credit: Barwon Valley Stainless

This article is featured in Australian Stainless Magazine issue 70, 2020.

Stainless at first sight

Located in the foothills of Perth, Aegis Amherst opened in July 2019 providing residential aged care in Canningvale, Western Australia. Set at the core focal point of the aged care facility presents a grand stainless steel balustrading ramp façade. 

ASSDA Member and Accredited Fabricator Balustrading WA were engaged by Absecon to fabricate and install a modern, safe, purpose-built ramp that would encompass strength and aesthetic attributes. 

The custom-designed ramp features an impressive 170 metres of grade 316 stainless steel tube. 

The handrails were manufactured from 50mm diameter stainless steel round tube. All stainless steel components were specified with a No. 7 high polish finish, supplied by several local suppliers including ASSDA Member, Stirlings Performance Steels. Mild steel flat bar was also used as the infill panels. Grade 316 stainless steel was specified primarily for its longevity, aesthetic appeal, and material strength. In addition, it is a durable and long-lasting alternative to competing materials.

Balustrading WA were heavily involved in the design brief and process, due to the extensive curvature inherent in the site. A range of advanced surveying techniques had to be used to ensure the balustrading was fabricated and installed correctly. This included using 3D image scans set into GPS grid location co-ordinates, rather than manual site measuring or templating as with more straightforward designs. As an example, the stainless steel support posts were scanned and fabricated individually to size to ensure correct fitment. In total, the project took just over 12 months to complete. 

The stainless steel ramp reflects the aged care’s cornerstone of their philosophy, by providing their residents with an environment that is comfortable and safe while delivering an aged care that helps them lead active, mobile and healthy lives.

This striking ramp facade continues to be the “hero” image for the facility, as stainless steel has once again delivered in compliance and material strength while fulfilling design and aesthetic needs.

     

Photo credit: Balustrading WA

This article is featured in Australian Stainless Magazine issue 70, 2020.

A stainless approach to protecting the environment

Safeguarding Australia’s environmental biosecurity is critical in preventing the introduction and spread of pests and diseases, and the Post Entry Quarantine (PEQ) facility in northern Melbourne is setting the benchmark in international best practice with the use of stainless steel.

The PEQ facility in Mickelham is a state-of-the-art, purpose-built operation constructed to streamline the country’s quarantine services and consolidate five pre-existing Commonwealth PEQ facilities spread across New South Wales, Victoria, South Australia and Western Australia. Managed by the Department of Agriculture and Water Resources, the 144ha site includes an administration building, modern laboratories, dog and cat receiving areas, horse facilities and separate compounds for birds, ruminants, bees, plants, horse veterinarians and dogs and cats. Today, as Australia’s flagship quarantine control centre, the integrated PEQ facility is the first point of entry for all imported animals, plant material and insects entering the country, providing secure accommodation and biological containment.

One of the more challenging aspects of the PEQ facility’s construction was the design and build of the avian compound. The complex and demanding brief included the delivery of five high-criticality biocontainment units under Quarantine Containment Level 3 (QC3) requirements, the highest level of biosecurity containment. Containment of micro-organisms and prevention of their release is of utmost importance. Mitigating and eliminating risk of exotic pathogens and disease connected to avian imports such as fertile eggs and live birds is critical.

In association with UK-based Suncombe Engineering, a worldwide leader in the field of wastewater decontamination, ASSDA Member Fineweld Stainless Steel was engaged by hydraulics contractor Geschke Plumbing to supply, manufacture, and install the wastewater decontamination plant system and connecting containment pipework for the treatment of QC3 biowaste products in the avian compound.

The wastewater decontamination plant system required a 12,500L collection vessel and 1,750 heat treatment vessel, and the collection vessel was fabricated from 316 grade and the treatment vessel from 2205 duplex stainless steel with a 2B 0.6μm finish in Fineweld Stainless Steel’s Carrum Downs workshop. Following manufacture, the treatment vessel was packaged and transported to Suncombe Engineering in the UK for final assembly into the wastewater decontamination plant and to undergo a complete Factory Acceptance Test (FAT) as a certified testing authority. The wastewater decontamination plant was then transported back to Fineweld Stainless Steel in Australia for pre-testing at their facility and then installation on site.

In addition to the two vessels, Fineweld Stainless Steel installed and welded the connecting pipework on site, manufactured from 5t of 316 grade stainless steel. All pipework welded joints – approximately 1,500 butt welds – were orbital welded and each one inspected, tested and recorded as part of the project scope to comply with the client’s strict QC3 requirements. QC3 facilities use gaseous decontaminants including vaporised hydrogen peroxide and chlorine dioxide. The use of stainless steel offers material strength, hygiene and resistance to both corrosion and the chemicals required to deactivate pathogens, whilst ensuring a gas-tight system for fumigable ductwork.

The installation took place two stories underground, therefore manufacturing and pre-spooling had no margin of error. Extensive logistical challenges were diligently managed, and in collaboration with Suncombe Engineering and Geschke Plumbing, the project was delivered on-time and on budget by the Fineweld Stainless Steel team.

In what would have been traditionally manufactured and imported from overseas suppliers, Fineweld Stainless Steel is showcasing the high quality and technical capability of Australian stainless steel manufacturing, producing high-end pressure vessels and complex works for a demanding and precise application. World-class infrastructure demands high quality products and long-term asset performance, both of which have been successfully delivered for the avian compound of Mickelham’s PEQ Facility through superior local workmanship and the use of stainless steel.

 

 

Photo credit: Geschke Plumbing

This article is featured in Australian Stainless Magazine issue 69, 2020.

 

Coloured and patterned stainless steel

Think stainless steel, and most people think ‘bright, shiny and silver’. But did you know that specifying stainless steel is not limited by its silver appearance?

Coloured and textured stainless steel is an exciting material choice for designers and architects. In addition to offering a high quality and aesthetically-pleasing finish with choice of colour, stainless steel’s superior benefits when compared with plastics or anodised aluminium include resistance to heat, light, abrasion and corrosion, and overall increased durability and performance extending the service life of the application.

This article will take a look back at the development of coloured stainless steel, detail the electrochemical colouring and PVD coating processes, and explore the various surface textures available.

History and development

Back in late 1960s, INOX developed a process for uniformly colouring smooth stainless surfaces. The colour relied on the growth of a uniform oxide-based film in a sulphuric and chromic acid mixture. The colour changed because of the interference of reflections from the top of the layer and the metal underneath it. It is like the colours in a soap bubble or an oil film, except that the INOX film had a very uniform thickness. This is because it is grown under uniform temperature and flow conditions with tightly controlled chemistry. Because the colours were subtractive rather than additive, they were not the same as a rainbow spectrum, but colours ranged through bronze, blue, black, charcoal/grey, gold, purple and green as the film grew from 20nm to 360nm. The colours also varied slightly with viewing angle because of the interference process that gives the colour.

Initially, there were two limitations and two caveats. Firstly, the coatings were easily abraded so it should not be used in heavily trafficked areas because any mechanical damage could not be repaired. Secondly, it was initially only grown on 304. And the caveats? The tight thickness limits mean that batch-to-batch colours could have slight tint variations although, this also has been exploited to provide a softer colour image.

Electrochemical colouring

Within a decade, a dual stage process was developed with an electrochemical treatment that provided greater abrasion resistance. Research in Australia showed that, for 304 base material, the film provided a slight improvement in corrosion resistance although the change is not as significant as a passivation process. Further developments showed that coloured films could also be formed on 316. The necessity for a uniform film thickness still requires factory treatment which means that it is limited to sheets or round surfaces such as tubes. Nevertheless, building facades, shopping centres and smooth surfaced art works were able to display a variety of stainless steel colours, even when the coloured stainless steel has been carefully bent into shapes.

These colours are very durable, even in Australia, as they do not fade with UV exposure and, in a graffiti-infected urban environment, solvents can be used to remove tags and other unwanted additions to coloured facades and signs. However, they are not repairable if scratched and can only be mechanically fixed as welding locally destroys the coloured film.

Surface Blackening

Do the arms of your black windscreen wipers use this colouring process? Well, no. The rich, glossy black used to be from immersion of stainless steel in molten sodium/potassium dichromate at 400oC for about 30 minutes but is now usually replaced by a 180oC cured organic coating. Shorter immersion times were used for thermal solar water heaters but they are now either painted or plastic - although black chrome has had a place in the market. 

Physical Vapour Deposition (PVD) coating

The second major method of colouring stainless steel is PVD or Physical Deposition of a Vapour – hence PVD. The process is carried out in a high vacuum chamber with a small amount of (usually) argon gas. The gas is ionized by a high negative voltage on the target and forms a plasma of electrons and positive ions which bombard the source metal and ejects (or sputters) metal ions or atoms. These are deposited on the product to form a thin (typically 300nm) coating on the clean product. It is critical that the coated surface is free from contaminants or the coating will lack adhesion. It is routinely used to hard coat small objects like drills but, on a larger scale it produces coloured door furniture or objects whose size is only limited by the vacuum chamber. Coating larger objects and sheet material requires greater electron ionization efficiency in the plasma which typically uses magnetic fields parallel to the surface of the target. 

The source metal can also be generated by thermal evaporation but this is less common.

Unlike the electrochemical INOX process, the colour of the PVD coating is determined by the source material with a few examples shown in the table. It is also invariant with viewing angle. PVD coatings are much more abrasion resistant than the INOX system but are not indestructible. 

Patterned stainless steel: Surface texture and its effect

A range of embossed, patterned and textured stainless steel finishes are available. Hot rolled finishes are usually too dimpled for aesthetic finishes. Cold rolled mill finishes are smooth and either dull grey (2B) or very bright (BA – bright annealed) and provide differing basic appearances but the same mechanical properties. Both have significantly better corrosion resistance than as-abraded finishes. Aesthetic changes by abrasion or blasting will provide feature finishes but have only minor effects on the colour and mechanical properties although rough 

as-abraded surfaces are known to be less corrosion resistant, i.e. the 0.5 micrometre Ra criterion.

Mechanically embossed profiles on austenitic mill rolled finishes might reduce the cleanability, but they also increase the strength because of cold work strengthening - while retaining the base metal corrosion resistance. This strengthening means that thinner material can be used, such as the thin checker sheet used in toolboxes – good visuals and lower weight in the utility with security for tools. Profiled sheet for outdoor public seating is another application with thinner sheet because of the strength and a bright appearance without glare.

High wear areas such as airport baggage collection or hospital corridors often use rigidised stainless steels where a through sheet profile significantly increases strength and stiffness with a pleasing aesthetic. An added advantage for profiled finishes is that scratches only affect the peaks and are less apparent partly because they are not continuous. On a grander scale, the Petronas Towers in Kuala Lumpur, Malaysia is a more complicated Cambric profiled finish on a base 316 metal with BA stock. The profiled finish is to avoid blinding reflections while using a 316 base metal with a mill finish that has the highest corrosion resistance available.

 

Bus station seat with colourful anodised aluminium arms

Petronas Towers in Kuala Lumpur, Malaysia
Photo credit: Outokumpu

University of Florida (UF) Health Shands Children’s Hospital
Photo credit: International Stainless Steel Forum (ISSF)

Banner image - Westfield Doncaster, Victoria
Photo credit: Steel Color Australia

This article is featured in Australian Stainless Magazine issue 69, 2020.

 

Rheem Australia’s Sturdy Stainless Steel Range

Stainless steel hot water heaters offer superior design combining high thermal efficiency, corrosion resistance, durability and performance for domestic applications.

ASSDA Member Rheem Australia has been committed to delivering hot water systems for over 80 years, with its first gas water heater manufactured in 1939 in Waterloo, Sydney. Through new product development and innovation, Rheem Australia has pioneered the commercial production of Australian-made hot water systems, designed and built for Australian conditions.

Operations Manager at Rheem, Gavan Schaeche, says, “Rheem Moorabbin is leading the way with its very own Stainless Steel and Commercial Centre of Excellence. The centre performs 125km of stainless steel welds a year to keep up with the demand of the new range which has quickly become an industry favourite.”

Rheem Australia’s stainless steel hot water system range includes gas and electric storage ranging in capacities from 50L to 315L. Manufactured from a range of stainless steel grades, the hot water systems use mains pressure water delivery and do not require a sacrificial anode for corrosion protection, reducing long-term maintenance and service costs over the life of the water heater.

The electric stainless steel models in the hot water system range offer high energy efficiency, exceeding Minimum Performance Standards (MEPS) by 12-24%. In addition, stainless steel cylinders weigh significantly less than comparable vitreous enamel models, making the product easier to manoeuvre and install. It is particularly well-suited for households that have their water heater installed indoors or in elevated multi-storey locations. 

Victorian-based Plumber and Founder of The Tap Man, Chris Arms, has been providing household solutions for thirty years. Delivering reliable household appliances is paramount to maintaining a highly satisfied client base, and when Chris receives a request to replace a hot water system, he always recommends the most suitable product from the Rheem stainless steel range. 

“I like to bring my customers along on the journey to find the right solution for their home through education about what they can expect from the products and materials I’m installing.

While the stainless steel range comes at a higher price point, it’s absolutely worth the investment. In my experience, stainless steel is a robust material that’s durable, corrosion resistant and less likely to incur a leak,” Chris says.

“It’s also one of the only hot water systems where I often do a repair over a replacement, should there be an issue such as an element assembly requiring replacement. The stainless steel tank makes a repair worthwhile.”

Stainless steel can present a higher upfront cost when comparing various hot water system products, however its investment is surpassed by the material’s performance and lifespan, and cost savings in energy efficiency, service and maintenance costs.

 

This article is featured in Australian Stainless Magazine issue 69, 2020.

 

Stainless steel… Limitless

‘Limitless’ is the stainless steel sculptural creation of Gold Coast artist Ian Haggerty, whose concept was selected in a design competition by Bond University to celebrate their 30th anniversary.

The 6.5m tall sculpture takes pride of place under the university’s iconic Arch and gleams in dignity and elegance from its 316L grade stainless steel construction. Inspired by the limitless possibilities created by education, the sculpture features a world sphere at its centre with four overarching wings representing the four pillars of learning: Learning to know, learning to do, learning to live together, and learning to be.

Reflection was also a key concept in the sculpture’s design, with mirror polished stainless steel the unrivalled material choice in bringing together the alumni and future students to inspire and signify that there are no limitations to education when it comes to gender, age, race, or religion.

In a nod to celebrating local fabrication, the artist engaged Burleigh-based ASSDA Member and Accredited Fabricator Atlas Stainless Balustrade & Fabrications to fabricate and install the 1.5t sculpture. 

Stainless steel rings were laser cut in various sizes from 100kg of 5mm mirror polished plate and welded together to create the intricate bubble pattern featured in the top section of the four wings. The bottom sections were fabricated from 400kg of plasma cut plate, with 1mm sheeting used to cover the bottom eight sides to allow for the chemical etching of over 26,000 Bond University graduates in homage of their educational achievements.

The Atlas Stainless Balustrade & Fabrications team also fabricated the base structure, and sphere and wing supports from mirror polished pipe to bring together the pre-constructed world sphere and its overarching wings. The fabrication process involved the team using their in-house plasma cutter, CNC bandsaw, CNC section roller and in-house polishing equipment both by machine and hand, and specialist welding techniques.

The project took over six months to complete and the structure was installed using two cranes, joining the university’s existing landmarks as a focal point of the state-of-the-art campus landscape. Special lighting effects were also installed as part of the sculpture to highlight its key features at night and shimmer in the surrounding water of the lake fountain.

‘Limitless’ was unveiled in May 2019 to celebrate the university’s 30-year milestone and remains a legacy piece for Bond University.  

This article is featured in Australian Stainless Magazine issue 69, 2020.

 

Stainless for  winemaking success

A growing demand for quality wines in China has seen its third-largest winemaker venture onto Australian soil with a new state-of-the-art winery incorporating over 800t of stainless steel. 

Weilong Wines’ winery in Red Cliffs, Northern Victoria is the first Australian winery development of its magnitude for many years, and the company’s investment in the Murray-Darling region is a testament to the strong reputation and quality of Australian wine. Grape crushing for the export-only wine has already commenced following the completion of the winery’s construction in March 2019 and is expected to have wine bottled before the year-end in time for the Chinese New Year celebration in January 2020.

ASSDA Member and Accredited Fabricator A&G Engineering designed, manufactured, delivered and installed all stainless steel storage and processing vessels for the new winery. The project scope was to achieve a vintage intake of over 26,000t capacity of grapes, equating to 21 million litres of wine.

Stainless steel was selected as the material of choice for the wine production equipment because of its excellent corrosion resistant properties, durability and ease-of-cleaning. Furthermore, the use of stainless steel does not impart additional flavour to the wine, preserving the original palates offered in the grape.

A total of 180 stainless steel tanks in grade 304/304L were delivered - 124 storage vessels ranging from 30kL to 1200kL, 42 fermentation vessels and 14 general processing tanks - plus associated stair towers, platforms, catwalks, support structures and connections.

Over 700t of 2mm-6mm stainless steel coil was supplied for the project by ASSDA Member, Outokumpu. In addition, the A&G Stainless Steel Sales Department was engaged to supply over 15km of primarily 304 grade tube in sizes ranging from 20mm to 300mm, plus all associated fittings.

Two 1200kL storage vessels were manufactured by A&G on site, using their own fully automated Plasma TIG welding process for tank manufacture, Site PAM (Precision Automated Manufacturing). The unique system was designed with a focus on large-capacity stainless steel vessels being constructed in the field, giving A&G the capability to custom build vessels that hold in excess of 5 million litres. 

Site PAM’s automatic planishing system compresses the weld with high pressure to ensure there are no peaks inside or outside of the tank, providing an aesthetically pleasing finish and a flat surface for the automated polishing application. All vessels were passivated for added corrosion resistance.

With safety and logistical considerations managed, 24-hour shifts were undertaken to fabricate the two 1200kL tanks to minimise downtime and maximise the efficiency of the project planners and estimators’ time on site.

The fabrication of the remaining 178 stainless steel storage vessels were spread across A&G’s three workshop premises, including Griffith in New South Wales, Mildura in Victoria and Angaston in South Australia. The extensive logistical challenges were managed with diligent project management, forward planning and transparency across the three sites and different production teams.

Transportation of the larger storage vessels required National Heavy Vehicle Regulator road permits, allowing only small pre-set time windows and significant planning to ensure loading and unloading occurred as planned to meet the scope of the permit. All vessels were delivered on A&G’s specialised tank trailers, and the larger vessels were transported on trailers specifically designed for the operation to comply with road regulations and permit requirements.

A&G was also appointed as the WH&S Principal Contractor for its portion of the works, taking responsibility and liability for all safety aspects on those parts of the site under its control. With the complexity of works being undertaken day-to-day, including the use of cranes up to 100t, heavy materials, working at heights, hot works, traffic management, job safety analysis requirements and standard operating procedures, the breadth of safety considerations were significant. Zero injuries or notifiable incidents were recorded over the duration of the ten-month project on site, a fantastic result given the magnitude of the project.

The end result is a technologically-advanced, modern winery with state-of-the-art stainless steel equipment and infrastructure built to last. With China continuing to drive growth and demand for wine imported from Australia, Weilong Wines plan to expand production each year, with the potential for future capacity to reach 168,000t per annum.

Immerse yourself in stainless luxury

Setting the benchmark in boutique luxury and innovation using stainless steel is Brisbane’s Emporium Hotel.

Developed by the Anthony John Group, The Emporium Hotel opened in July 2018. Nestled in the premier lifestyle and cultural precinct of South Bank, the 143-suite hotel is turning heads with its exquisite interior design, bespoke handcrafted features and luxurious facilities.

Stainless steel was the material of choice for the five-star hotel and selected for its quality, opulent aesthetic and luxury appeal. Over 5.5 tonnes of grade 304 stainless steel sheet, 1.2mm thick in a No. 8 mirror finish was used throughout the five-star hotel and supplied by ASSDA Member Fagersta Steels

ASSDA Member and Accredited Fabricator, Langford Metal Industries, was engaged to laser cut the mirror finish material to bring the developer’s trademark design to life, which was installed by Thump Architectural.

The frangipani inspired pattern represents the Queensland theme and character, and the laser cut stainless steel prevails throughout the hotel on mullions, sliding doors, external panels, columns, cabana suites surrounding the 23m infinity edge pool – almost anywhere and everywhere, serving both a functional and decorative purpose.

A remarkable feature of the hotel is its rooftop bar on the 21st floor, The Terrace. Presenting panoramic views of South Bank Parklands, the Brisbane River and the city skyline, The Terrace maximises the warm Queensland weather with two retractable roofs offering full, partial or no exposure.

Measuring 7.5m long, 2.1m wide and 50mm thick, the ceiling of the first retractable roof features the impressive frangipani stainless steel design. The sliding panel is a composite structure incorporating insulation and structural members which are clad top and bottom with mirror polished stainless sheet. For structural purposes, the panel was shaped into a shallow moon profile to form the roof’s arch. When retracted, a second roof made of glass is revealed, which is also retractable for a complete outdoor rooftop experience.

The stainless steel ceiling and surrounding elements complement the rooftop bar’s sub-tropical luxe vibe with ceiling-to-floor glass doors, lush greenery, and white backlit onyx floor tiles and bar.

 

Photo Credit: Emporium Hotel

Coastal living

Stainless Steel Pool Fencing

Safety is the number one consideration when building a pool fence, and stainless steel delivers in compliance and material strength while fulfilling design and aesthetic needs.

A stunning canal-front home on the Gold Coast features a streamlined stainless steel vertical balustrade system as supplied by ASSDA Member Miami Stainless.

The custom-designed stainless steel pool fence features 50mm square mirror-polished posts and upper and lower rails. Complying with Queensland pool fencing and safety barrier regulations, the vertical stainless steel wire balustrades were spaced 80mm apart and installed using Miami Stainless’ Nutsert Swage Stud System on the base with a ProRig Flip Toggle into the handrail.

Grade 316 stainless steel was specified for its aesthetic appeal, material strength and corrosion resistance, particularly with the home’s waterfront location and close proximity to the coastline.

In addition, stainless steel is a durable and long-lasting alternative to aluminium balustrades and offers reduced household maintenance when compared with glass. Glass fencing often requires frequent cleaning to remove chlorine or saltwater splashes and finger marks. 

The stainless steel pool fence ticks all the boxes in combining safety, unobstructed views, durability, minimal maintenance and luxury style.

 

Photo credit: Miami Stainless

 

Shielding gases for welding and their effects on stainless steel properties

Shielding gases form an integral part of all conventional welding processes. 

They serve multiple functions but are primarily there to shield the weld pool from the atmosphere and to provide a medium which can allow the flow of electricity from an electrode to a workpiece. Even processes that do not have an external gas supply such as Manual Metal Arc Welding (MMAW or MMA or SMAW) and Gasless Flux-cored Arc Welding (FCAW) all have a shielding gas which is generated by the decomposition of the flux in the presence of the welding arc.

The shielding gas can also have an effect on arc stability, weld shape and depth of penetration as well as the mechanical properties and metallurgy of stainless steel weldments.

The gas shielded processes such as Gas Tungsten Arc Welding (GTAW or TIG) and Gas Metal Arc Welding (GMAW or MIG) use shielding gases of a variety of compositions depending on the application. As the electrode in GTAW is made of tungsten, the shielding gas is typically argon or helium to prevent oxidation of the electrode. This restriction does not apply to GMAW and therefore the gas composition may include active gases such as carbon dioxide and oxygen. Small quantities of other gases such as nitrogen and hydrogen can be utilised with both of these processes as they are particularly advantageous for the welding of stainless steel. While neither gas is inert by definition, they can be used with GTAW as neither react with tungsten.

There are three key properties of the shielding gas which control the way the weld pool behaves; the ionisation potential (how easily an atom will give up an electron), the thermal conductivity of the gas, and finally the surface tension between the weld pool and the shielding gas.

Ionisation potential

The shielding gas allows transfer of electrons between the electrode and the workpiece. Upon arc initiation, electrons are emitted from either the workpiece or the electrode depending on which is positively charged. These electrons collide with gaseous atoms which results in these atoms liberating one of their electrons which results in a chain reaction that sustains the arc. The ionisation potential of the gas is the ease with which they will give up an electron. ‘Hotter’ gases are those which require more energy to ionise or release an electron. Helium has a higher ionisation potential than argon, so has a higher arc voltage and hence a higher heat input for the same current and arc length. 

A similar principle applies to molecular gases (H2, N2, O2, CO2) which dissociate in the arc into individual atoms and then recombine upon cooling, releasing energy in the process. Argon is often mixed with small amounts of other gases to improve weld penetration.

Thermal conductivity

The thermal conductivity of a shielding gas affects its ability to transfer heat across the arc. It influences the radial heat loss from the centre to the periphery of the arc column as well as heat transfer from the arc to the molten weld pool. Gases with low thermal conductivity such as argon will tend to have a narrow hot core in the centre of the arc and a considerably cooler outer zone. The result is a weld with a narrow ‘finger’ at the root of the weld and a wider top. On the other hand, helium has a high thermal conductivity, so heat is more evenly distributed across the arc, but as a result the depth of penetration is lower. Mixing gases allows combination of the advantageous properties of each gas while limiting the drawbacks.

 

 Surface tension

Surface tension affects the bead profile of a weld. Picture how water beads up on a newly polished car. This is undesirable in welding as it creates a steep angle between the weld and the parent which could lead to defects such as undercut, lack of sidewall fusion and decreased fatigue performance. This is another reason why pure argon is not used as a shielding gas for the GMAW process. 

Gas components

Oxygen

Though seemingly counterintuitive as it is well known that hot metals oxidise, small amounts of oxygen are often added to shielding gasses for the GMAW process. Small amounts of oxygen reduce the surface tension between the molten weld pool and the surrounding atmosphere. Lower surface energy results in a flatter and smoother weld bead with less tendency to undercut the parent metal. To minimise alloy losses by oxidation, oxygen content is typically limited to 2%. The heat tint will be more severe than for a weld without oxygen additions to the shielding gas.

Carbon Dioxide

GMAW also utilises CO2 as a constituent of the shielding gas. A common concern with stainless steels is embrittlement and corrosion through sensitisation due to chromium carbide formation, but the carbon pickup from CO2 has been demonstrated to be low enough that the resultant weld metal still achieves the required (≤0.03%) carbon content for L grade designation. The chosen CO2 content is therefore more about penetration and wetting than it is about carbon pick-up. Carbon dioxide contents in GMAW are typically 2-5% while flux-cored wires utilise 20% mixtures with argon or even 100% CO2

Hydrogen

Unique to austenitic stainless steels is its immunity to hydrogen cracking – except possibly in very heavily cold-worked material. This allows the addition of hydrogen to the shielding gas in quantities from 2–15% providing more heat in the arc and better penetration. Hydrogen quantity for manual welding is usually restricted to 5%, with the higher concentrations limited to automated process such as orbital GTAW. Hydrogen cannot be used as a component of the shielding gas for ferritic, martensitic or duplex stainless steels due to a risk of cracking. 

Nitrogen

Nitrogen is a useful shielding gas additive for duplex stainless steels which contain dissolved nitrogen. It is added to increase pitting resistance and in acting as an austenite stabiliser to create a balanced ‘duplex’ microstructure in the weld, especially for thin materials which cool too rapidly to allow sufficient austenite to form. Nitrogen can be added to both the welding gas and the purge gas to prevent the loss of nitrogen during welding.


This article has dealt with gases for the active side of a weld. When welding tube or pipe, it is normal to feed an inert gas such as argon or nitrogen into the tube or pipe to maintain low oxygen levels and minimise heat tint formation to no more than pale straw. This usually requires a sensitive oxygen meter or possibly previously proven purging practices. In thick sections, purging must continue for all passes. Nitrogen purging of duplex root passes will improve the corrosion resistance but may also upset the phase balance. Hydrogen additions have been used in purge gases for both austenitic and duplex welds to minimise heat tints.