Stainless steel has delivered the confidence it will provide the structural performance and meet the 100-year life-cycle of a new marina development on the New South Wales’ South Coast.
The Waterfront, Shell Cove, is a joint residential and mixed-use development between Shellharbour City Council and Frasers Property Australia located 22km south of Wollongong.
Central to the development is its waterfront location and world-class marina that will offer pontoon berthing for approximately 270 vessels, direct access to the Pacific Ocean, charter boat operations, a public boat ramp and a variety of marina facilities and services.
Stainless steel reinforcement has played a